CAMPUS® datasheet | PEBAX MX 1205 SW 2


This datasheet of PEBAX MX 1205 SW 2 from ARKEMA is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  PEBAX MX 1205 SW 2 | TPA | ARKEMA
Product Texts
POLYETHER BLOCK AMIDE (PEBA)
PEBAX
hardness 40 shore D
Non plasticized flexible Polyamide
Outstanding mechanical properties at low temperature (-40°C)
Applications : molded parts for sport goods (softness, 
        nice touch feeling ...)
        Industrial (damping properties, overmolding, 
        resiliency...)
Rheological propertiesdry / condUnitTest Standard
Molding shrinkage (parallel) 0.4 / * % ISO 294-4, 2577
Molding shrinkage (normal) 1.1 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 88 / 81 MPa ISO 527-1/-2
Stress at 50% strain 7 / 7 MPa ISO 527-1/-2
Stress at 10% elongation 6 / * MPa ISO 527-1/-2
Stress at 100% elongation 9 / * MPa ISO 527-1/-2
Stress at break TPE 42 / * MPa ISO 527-1/-2
Strain at break >50 / >50 % ISO 527-1/-2
Strain at break TPE >300 / * % ISO 527-1/-2
Charpy impact strength (+23°C) - / N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) - / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) - / N kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) - / N kJ/m² ISO 179/1eA
Compression Set under constant strain (23°C) 37 / * % ISO 815
Tear strength 77 / * kN/m ISO 34-1
Abrasion resistance 40 / * mm³ ISO 4649
Shore D hardness (15s) 41 / * - ISO 868
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 147 / * °C ISO 11357-1/-3
Temp. of deflection under load (0.45 MPa) 52 / * °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
Electrical propertiesdry / condUnitTest Standard
Relative permittivity (100Hz) 9 / - - IEC 60250
Relative permittivity (1MHz) 6 / - - IEC 60250
Dissipation factor (100Hz) 2090 / - E-4 IEC 60250
Dissipation factor (1MHz) 1120 / - E-4 IEC 60250
Volume resistivity 1.60E11 / - Ohm*m IEC 60093
Surface resistivity * / 3E12 Ohm IEC 60093
Electric strength 43 / - kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.2 / * % Sim. to ISO 62
Humidity absorption 0.4 / * % Sim. to ISO 62
Density 1010 / 1010 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 830 kg/m³ -
Thermal conductivity of melt 0.18 W/(m K) -
Spec. heat capacity melt 2500 J/(kg K) -
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 220 °C ISO 294
Injection Molding, mold temperature 30 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 30 MPa ISO 294
Diagrams
Viscosity-shear rate , PEBAX MX 1205 SW 2, TPA, ARKEMA
Shearstress-shear rate , PEBAX MX 1205 SW 2, TPA, ARKEMA
Stress-strain , PEBAX MX 1205 SW 2, TPA, ARKEMA
Secant modulus-strain , PEBAX MX 1205 SW 2, TPA, ARKEMA
Specific volume-temperature (pvT) , PEBAX MX 1205 SW 2, TPA, ARKEMA
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Other Extrusion, Transfer Molding, Casting, Thermoforming
Delivery form
Pellets
Special Characteristics
Platable, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat, Transparent
Regional Availability
Other text information
Injection molding
PREPROCESSING

Max water content:      0.03 - 0.15     %

Notice text      :      Our products are delivered pre-dried and in sealed
                 :      bags.Therefore, they do not require any drying
                 :      stage before use:

                 :      1- Keep the bags at the workshop temperature for
                 :         several hours before use.

                 :      2- Re-dry the product whenever the bags have
                 :         remained open for more than 4 hours.

PROCESSING

Melt temperature :      180 - 240       °C
Mold temperature :       20 -  40       °C

Notice text      :      Under specific conditions, our product can easily 
                 :      withstand 20 to 30 degrees more than the
                 :      recommended temperatures.

Film extrusion
PREPROCESSING
 

Max water content:      0.03 - 0.15     %

Notice text      :      Our products are delivered pre-dried and in sealed
                 :      bags.Therefore, they do not require any drying
                 :      stage before use:

                 :      1- Keep the bags at the workshop temperature for
                 :         several hours before use.

                 :      2- Re-dry the product whenever the bags have
                 :         remained open for more than 4 hours.

PROCESSING
     :

Melt temperature :      190 - 220       °C

Other extrusion
PREPROCESSING
 

Max water content:      0.03 - 0.15     %

Notice text      :      Our products are delivered pre-dried and in sealed
                 :      bags.Therefore, they do not require any drying
                 :      stage before use:

                 :      1- Keep the bags at the workshop temperature for
                 :         several hours before use.

                 :      2- Re-dry the product whenever the bags have
                 :         remained open for more than 4 hours.

PROCESSING
     

Melt temperature :      160 - 180       °C
Profile extrusion
PREPROCESSING
 

Max water content:      0.03 - 0.15     %

Notice text      :      Our products are delivered pre-dried and in sealed
                 :      bags.Therefore, they do not require any drying
                 :      stage before use:

                 :      1- Keep the bags at the workshop temperature for
                 :         several hours before use.

                 :      2- Re-dry the product whenever the bags have
                 :         remained open for more than 4 hours.

PROCESSING
     

Melt temperature :      150 - 180       °C

Notice text      :      Due to elastic behaviour of this grade, it is
                 :      necessary to usea special sizing device.Contact
                 :      us for more information.

                 :      Too high temperatures can generate sticking of the
                 :      melt on the sizer.

Sheet extrusion
PREPROCESSING
 

Max water content:      0.03 - 0.15     %

Notice text      :      Our products are delivered pre-dried and in sealed
                 :      bags.Therefore, they do not require any drying
                 :      stage before use:

                 :      1- Keep the bags at the workshop temperature for
                 :         several hours before use.

                 :      2- Re-dry the product whenever the bags have
                 :         remained open for more than 4 hours.

PROCESSING
     :

Melt temperature :      190 - 220       °C
Disclaimer

This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991