Productprofil:
PLEXIGLAS® Optical POQ66 is an amorphous thermoplastic molding compound based on polymethyl methacrylate (PMMA).
In addition to the familiar properties of PLEXIGLAS® molding compounds, such as
- excellent light transmission and brilliance,
- very good weather resistance,
- high mechanical strength, surface hardness and mar resistance,
PLEXIGLAS® Optical POQ66 is distinguished by its
- guaranteed purity and clarity,
- high luminous efficiency in medium to long light paths,
- absolute colorlessness even in thick layers.
Application:
PLEXIGLAS® Optical POQ66 is suitable for manufacturing extruded sheets to meet stringent optical requirements.
Example:
Small to medium-sized injection-molded or injection compression-molded lightguide panels for display applications, lightguides.
Processing:
PLEXIGLAS® Optical POQ66 can be processed on extruders with conventional three-section screws for engineering themoplastics.
For manufacturing extruded lightguide panels, it is advisable to maintain processing temperatures at the lower end of the scale.
Physical Form / Packaging:
PLEXIGLAS® Optical POQ66 is supplied as uniform pellets in big bags. Other forms of packaging on request.
| Rheological properties | Value | Unit | Test Standard |
| Melt volume-flow rate (MVR) | 2.9 | cm³/10min | ISO 1133 |
| Temperature | 230 | °C | ISO 1133 |
| Load | 3.8 | kg | ISO 1133 |
| Mechanical properties | Value | Unit | Test Standard |
| Tensile Modulus | 3200 | MPa | ISO 527-1/-2 |
| Stress at break | 69 | MPa | ISO 527-1/-2 |
| Strain at break | 4 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 20 | kJ/m² | ISO 179/1eU |
| Thermal properties | Value | Unit | Test Standard |
| Glass transition temperature (10°C/min) | 108 | °C | ISO 11357-1/-2 |
| Vicat softening temperature (50°C/h 50N) | 104 | °C | ISO 306 |
| Electrical properties | Value | Unit | Test Standard |
| Volume resistivity | >1E13 | Ohm*m | IEC 60093 |
| Other properties | Value | Unit | Test Standard |
| Density | 1190 | kg/m³ | ISO 1183 |
| Material specific properties | Value | Unit | Test Standard |
| Luminous transmittance | 92 | % | ISO 13468-1, -2 |
| Test specimen production | Value | Unit | Test Standard |
| Processing conditions acc. ISO | 8260 | - | ISO ....-2 |
| Injection Molding, mold temperature | 64 | °C | ISO 10724 |
| Injection Molding, injection velocity | 195 | mm/s | ISO 294 |
Predrying temperature: max. 94 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 260 °C
Die temperature: 220 - 260 °C
Predrying temperature: max. 94 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 260 °
Die temperature: 220 - 260 °C
All listed technical data are typical values intended for your
guidance. They are given without obligation and do not constitute a
materials specification. Should you have any further questions
concerning material behavior or properties, please contact us
at the following address :
Evonik Röhm GmbH
Marketing / Campus
Kirschenallee
D-64293 Darmstadt
Germany
Phone: +49 - (0) 61 51 / 18-47 11
Fax: +49 - (0) 61 51 / 18-31 77
E-Mail: campusplastics@evonik.com
Internet: http://www.plexiglas.net
® = registered trademark
PLEXIGLAS® is a registered trademark of Evonik Röhm GmbH, Germany,
outside of the Americas. Within the Americas it is sold as ACRYLITE®,
which is a registered trademark of Evonik Cyro LLC, USA.
PLEXIMID® is a registered trademarks of Evonik Röhm GmbH, Germany.
CYROLITE® and XT® polymer are registered trademarks of Evonik Cyro LLC, USA.
This information and all further technical advice is based on our present knowledge
and experience. However, it implies no liability or other legal responsibility on our part,
including with regard to existing third party intellectual property rights, especially
patent rights. In particular, no warranty, whether express or implied, or guarantee of
product properties in the legal sense is intended or implied. We reserve the right to
make any changes according to technological progress or further developments. The
customer is not released from the obligation to conduct careful inspection and testing
of incoming goods. Performance of the product described herein should be verified by
testing, which should be carried out only by qualified experts in the sole responsibility
of a customer. Reference to trade names used by other companies is neither a
recommendation, nor does it imply that similar products could not be used.
NAFTA:
This information and all technical and other advice are based on Evonik’s
present knowledge and experience. However, Evonik assumes no liability for
such information or advice, including the extent to which such information or
advice may relate to third party intellectual property rights. Evonik reserves the
right to make any changes to information or advice at any time, without prior
or subsequent notice. EVONIK DISCLAIMS ALL REPRESENTATIONS AND
WARRANTIES, WHETHER EXPRESS OR IMPLIED, AND SHALL HAVE NO LIABILITY
FOR, MERCHANTABILITY OF THE PRODUCT OR ITS FITNESS FOR A PARTICULAR
PURPOSE (EVEN IF EVONIK IS AWARE OF SUCH PURPOSE), OR OTHERWISE.
EVONIK SHALL NOT BE RESPONSIBLE FOR CONSEQUENTIAL, INDIRECT OR
INCIDENTAL DAMAGES (INCLUDING LOSS OF PROFITS) OF ANY KIND. It is the
customer’s sole responsibility to arrange for inspection and testing of all
products by qualified experts. Reference to trade names used by other
companies is neither a recommendation nor an endorsement of the
corresponding product, and does not imply that similar products could not be
used.
Sales range and technical data subject to alteration.CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991