CAMPUS® Datasheet | POLYFORT® FPP 20 T


This datasheet of POLYFORT® FPP 20 T from A. Schulman GmbH is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

POLYFORT® FPP 20 T | PP-T20 | A. Schulman GmbH
Product Texts
20% talc fillled PP homo polymer compound


Rheological propertiesValueUnitTest Standard
Melt volume-flow rate, MVR 8 cm³/10min ISO 1133
Temperature 230 °C ISO 1133
Load 2.16 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 2400 MPa ISO 527-1/-2
Yield stress 32 MPa ISO 527-1/-2
Yield strain 6 % ISO 527-1/-2
Nominal strain at break >50 % ISO 527-1/-2
Charpy impact strength, +23°C 41 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 17 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 4 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 3 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Temp. of deflection under load, 1.80 MPa 70 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 125 °C ISO 75-1/-2
Vicat softening temperature, 50°C/h 50N 95 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm IEC 60695-11-10
UL recognition UL - -
Electrical propertiesValueUnitTest Standard
Volume resistivity >1E13 Ohm*m IEC 60093
Surface resistivity >1E15 Ohm IEC 60093
Other propertiesValueUnitTest Standard
Density 1050 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate, POLYFORT® FPP 20 T, PP-T20, A. Schulman
Shearstress-shear rate, POLYFORT® FPP 20 T, PP-T20, A. Schulman
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion, Thermoforming
Delivery form
Granules
Regional Availability
Other text information
Injection molding
PREPROCESSINGPretreatment
Predrying usually not neccessary (2-4h / 80°C)

PROCESSINGProcessing:

Melttemperature230 - 270°C
Mouldtemperature40 - 70°C
The information and recommendations contained in this document are based upon
data collected by A. Schulman and are believed to be reliable; however, because
A. Schulman cannot anticipate or control the many different conditions under
which this information and/or product may be used, no representation is made
and no warranty is given of any kind, express or implied, for completeness,
accuracy, availability, suitability, usefulness, commercial value, or non-violation
of intellectual property rights of information, recommendations, and products
and services directly or indirectly provided. A. Schulman assumes no responsibility
for the results of the use of products and processes described herein and expressly
disclaims the implied warranties of merchantability and fitness for a particular use

If there are questions to given information, to further properties or further A. Schulman
products please contact

                  A. Schulman GmbH
                  Huettenstrasse 211
                  50170 Kerpen
                  Tel: 02273 / 561-0
                  Contact: aschulman@de.aschulman.com
                               Subject: Material data

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2014
 
Please drag slider to the right to unlock control points view