  POLYMAN® (ABS) E/HI | ABS-I | A. Schulman GmbH
Product Texts
High impact ABS for extrusion and injection moulding


Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 7 cm³/10min ISO 1133
Temperature 220 °C ISO 1133
Load 10 kg ISO 1133
Molding shrinkage (parallel) 0.4 % ISO 294-4, 2577
Molding shrinkage (normal) 0.4 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 1500 MPa ISO 527-1/-2
Yield stress 40 MPa ISO 527-1/-2
Yield strain 2.5 % ISO 527-1/-2
Nominal strain at break 20 % ISO 527-1/-2
Charpy impact strength (+23°C) N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 34 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 19 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Glass transition temperature (10°C/min) 102 °C ISO 11357-1/-2
Temp. of deflection under load (1.80 MPa) 88 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 93 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 90 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm IEC 60695-11-10
UL recognition UL - -
Electrical propertiesValueUnitTest Standard
Relative permittivity (100Hz) 3.2 - IEC 60250
Relative permittivity (1MHz) 3 - IEC 60250
Dissipation factor (100Hz) 120 E-4 IEC 60250
Dissipation factor (1MHz) 90 E-4 IEC 60250
Volume resistivity >1E13 Ohm*m IEC 60093
Surface resistivity >1E15 Ohm IEC 60093
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 1.2 % Sim. to ISO 62
Humidity absorption 0.3 % Sim. to ISO 62
Density 1030 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 940 kg/m³ -
Thermal conductivity of melt 0.15 W/(m K) -
Eff. thermal diffusivity 7.40E-8 m²/s -
Ejection temperature 100 °C -
Test specimen productionValueUnitTest Standard
Processing conditions acc. ISO 2580 - ISO ....-2
Injection Molding, melt temperature 250 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 10724
Injection Molding, injection velocity 250 mm/s ISO 294
Injection Molding, pressure at hold 100 MPa ISO 294
Diagrams
Viscosity-shear rate , POLYMAN® (ABS) E/HI, ABS-I, A. Schulman
Shearstress-shear rate , POLYMAN® (ABS) E/HI, ABS-I, A. Schulman
Specific volume-temperature (pvT) , POLYMAN® (ABS) E/HI, ABS-I, A. Schulman
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion, Thermoforming
Delivery form
Granules
Additives
Release agent
Special Characteristics
Platable
Regional Availability
Other text information
Injection molding
Pretreatment
Predrying: 3-4h / 80°C

Processing:

Melttemperature220 - 260°C
Mouldtemperature40 - 80°C

Disclaimer
The properties given in this software are typical, non-binding
mean values found fpor injection moulded natural coloured test
bars. Pigments and other modification may alter these values.
The characteristic values are based on our know-how and experience.
They do not warrant any specific properties. All our products
must be subjected to in house tests and inspections by the user
before application. This applies above all with regard to their
suitability for a particular purpose. It also applies accordingly
for all other written or verbal information given by our personnel.
Our General Terms of Business apply in all other respects,
particulaly with regard to liability for material defects.

If there are questions to given information, to further
properties or further A. Schulman products please contact

                  A. Schulman GmbH
                  Huettenstrasse 211
                  50170 Kerpen
                  Tel: 02273 / 561-0
                  Contact: Dipl.-Ing. M. Berg
                           aschulman@de.aschulman.com
                           Subject: Material data

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991