offers extended functionality!CAMPUS® datasheet | Pipelon® 401 NC010
This datasheet of Pipelon® 401 NC010 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
PIPELON® also has excellent mechanical properties and good resistance to fuels and oils. These properties make it an excellent candidate for pipes used to convey crude oil and refined products.
PIPELON® , a natural color resin, is under consideration for several applications in the Petroleum industry including liners for pipes carrying refined and semi-refined Petroleum products and core tubes for flexible risers and flow lines carrying crude oil, and spoolable high pressure water injection lines.
PIPELON® is an extrusion resin appropriate for liners, tubing and jacket applications requiring flexibility, as well as thermal and chemical resistance.
______________________________________________________
Pipelon® 401 is an unreinforced, flexible polyamide 612 for extrusion. It has excellent hydrolysis resistance, excellent dimensional stability, good temperature resistance, good chemical resistance and and is specifically suitable for use in tubes and pipes for the petroleum industry.
| Rheological properties | dry / cond | Unit | Test Standard |
| Molding shrinkage (parallel) | 2.4 / * | % | ISO 294-4, 2577 |
| Molding shrinkage (normal) | 2.2 / * | % | ISO 294-4, 2577 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 700 / 700 | MPa | ISO 527-1/-2 |
| Yield stress | 35 / 31.3 | MPa | ISO 527-1/-2 |
| Yield strain | 34 / 40 | % | ISO 527-1/-2 |
| Nominal strain at break | >50 / >50 | % | ISO 527-1/-2 |
| Charpy notched impact strength (+23°C) | 100 / 110 | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 212 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (1.80 MPa) | 51 / * | °C | ISO 75-1/-2 |
| Temp. of deflection under load (0.45 MPa) | 137 / * | °C | ISO 75-1/-2 |
| Coeff. of linear therm. expansion (parallel) | 170 / * | E-6/K | ISO 11359-1/-2 |
| Coeff. of linear therm. expansion (normal) | 110 / * | E-6/K | ISO 11359-1/-2 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Relative permittivity (100Hz) | 7.2 / 9.4 | - | IEC 60250 |
| Relative permittivity (1MHz) | 3.5 / 3.6 | - | IEC 60250 |
| Dissipation factor (100Hz) | 1300 / 1300 | E-4 | IEC 60250 |
| Dissipation factor (1MHz) | 500 / 900 | E-4 | IEC 60250 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 1.6 / * | % | Sim. to ISO 62 |
| Humidity absorption | 1 / * | % | Sim. to ISO 62 |
| Density | 1060 / - | kg/m³ | ISO 1183 |
| Film Properties | dry / cond | Unit | Test Standard |
| Dynamic coefficient of friction | 0.3 / * | - | ISO 8295 |
| Rheological calculation properties | Value | Unit | Test Standard |
| Spec. heat capacity melt | 2260 | J/(kg K) | - |
PREPROCESSING
Drying Recommended = Yes
Drying Temperature = 70°C
Drying Time, Dehumidified Dryer = 8h
Processing Moisture Content = < 0.05 %
PROCESSING
Melt Temperature Optimum = 230°C
Melt Temperature Range = 220-250°C
| Salt solutions | |
![]() | Zinc Chloride solution (50% by mass) (23°C) |
E.I. du Pont de Nemours and Company is pleased to provide information about its products with the CAMPUS electronic database.
The information provided is gratis and DuPont assumes no obligation or liability for any advice furnished or for any results obtained with respect to this information.
All such advice is given and accepted at the risk of the buyer. The disclosure of information herein is not an express or implied license to operate under any patent of DuPont or others.
DuPont warrants that the use or sale of any material which is described herein and is offered for sale by DuPont does not infringe any patent covering the material itself, but does not warrant against infringement by reason of the use thereof in combination with other materials or the operation of any process.
Unless otherwise noted, the property values are for natural color (NC010) resins only. Colorants or other additives may alter some or all of the properties.
The data listed herein fall within the normal range of product properties and they should not be used to establish specification limits nor used alone as the basis of design.
Material Safety Data Sheets (SDSs) can be obtained from local sales offices.
Products listed herein should not be used in medical applications involving permanent implantation in the human body or contact with internal body fluids or tissues unless the material has been provided from DuPont under a written contract that is consistent with DuPont policy regarding medical applications and expressly acknowledges the contemplated use.
For further information, please contact your DuPont representative.
You may also request a copy of DuPont policy regarding medical applications H-50103-2 and DuPont caution regarding medical applications H-50102-2.
Products listed herein may from time to time be modified or removed.
Please call your local sales office to determine current availability.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991