View list of
  • All BASF grades
  • All grades beginning with P

CAMPUS® datasheet | Polystyrol 495 F


This datasheet of Polystyrol 495 F from BASF is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  Pocan® TS 3220 | (PBT+PET)-I-GF20 | LANXESS Deutschland GmbH
Product Texts
PBT+PET, 20 % glass fibres, injection moulding, impact modified, low tendency to warp, improved surface finish
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 18 cm³/10min ISO 1133
Temperature 270 °C ISO 1133
Load 5 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 5600 MPa ISO 527-1/-2
Stress at break 80 MPa ISO 527-1/-2
Strain at break 3.5 % ISO 527-1/-2
Charpy impact strength (+23°C) 60 kJ/m² ISO 179/1eU
Puncture - maximum force (+23°C) 2.1 N ISO 6603-2
Puncture - maximum force (-30°C) 1.6 N ISO 6603-2
Puncture energy (+23°C) 2.7 J ISO 6603-2
Puncture energy (-30°C) 1.8 J ISO 6603-2
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 225 °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 155 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 215 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 150 °C ISO 306
Coeff. of linear therm. expansion (parallel) 30 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 130 E-6/K ISO 11359-1/-2
Other propertiesValueUnitTest Standard
Density 1360 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 270 °C ISO 294
Injection Molding, mold temperature 90 °C ISO 10724
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
This information and our  technical advice - whether verbal, in  writing
or by way of trials - are  given in good faith but without warranty, and
this  also  applies  where  proprietary  rights  of  third  parties  are
involved.  Our advice does not release you from  the obligation to check
its validity and to test our  products  as to their  suitability for the
intended processes and uses.  The  application, use  and  processing  of
our products and the products manufactured  by  you  on the basis of our
technical  advice  are  beyond our control and, therefore, entirely your
own  responsibility.  Our  products  are  sold  in  accordance  with our
General  Conditions of Sale and Delivery.
The values  stored in the databank should only be used as guidelines for
component   design.  In  giving  these  values  neither  guarantee,  nor
assurance of particular material properties can be given.

techcenter.lanxess.com

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991