  Powder D40 NATURAL | PA11 | ARKEMA
Product Texts
Powder D40 NATURAL - RILSAN POLYAMIDE 11 (PA11) POWDER



Unpigmented and clear Powder as an additive for paints.Improves the 
scratch and abrasion resistance of paints.Allows for different texture 
depending on the granulometry used.Can be dispersed completely in 
liquid media.

Excellent chemical resistance.

The range includes several colours.

The properties listed in the data base have been measured on a
corresponding RILSAN PA11 Granule.

Additional information is available from the sales network.
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 185 °C ISO 11357-1/-3
Vicat softening temperature (50°C/h 50N) 160 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
Burning Behav. at thickness h V-2 class IEC 60695-11-10
Thickness tested 3.2 mm IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
Volume resistivity 1E12 Ohm*m IEC 60093
Surface resistivity 1E14 Ohm IEC 60093
Electric strength 30 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Water absorption 1.9 % Sim. to ISO 62
Density 1040 kg/m³ ISO 1183
Characteristics
Processing
Coating
Delivery form
Powder
Regional Availability
Disclaimer

This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991