This datasheet of Powder T NAT BHV RX 2 from ARKEMA is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
Powder T NAT BHV RX 2 | PA11 | ARKEMA
Product Texts
Powder T NAT BHV RX 2 - RILSAN POLYAMIDE 11 (PA11) POWDER Unpigmented and clear Powder for the coating of printing rollers. Technical assistance available for any coating process problem. The range includes several colours. The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule. Additional information is available from the sales network.
| Thermal properties | Value | Unit | Test Standard |
| Melting temperature (10°C/min) | 185 | °C | ISO 11357-1/-3 |
| Vicat softening temperature (50°C/h 50N) | 160 | °C | ISO 306 |
| Burning Behav. at 1.5 mm nom. thickn. | V-2 | class | IEC 60695-11-10 |
| Thickness tested | 1.6 | mm | IEC 60695-11-10 |
| Burning Behav. at thickness h | V-2 | class | IEC 60695-11-10 |
| Thickness tested | 3.2 | mm | IEC 60695-11-10 |
| Electrical properties | Value | Unit | Test Standard |
| Volume resistivity | 1E12 | Ohm*m | IEC 60093 |
| Surface resistivity | 1E14 | Ohm | IEC 60093 |
| Electric strength | 30 | kV/mm | IEC 60243-1 |
| Other properties | Value | Unit | Test Standard |
| Water absorption | 1.9 | % | Sim. to ISO 62 |
| Density | 1040 | kg/m³ | ISO 1183 |
Characteristics
Processing
Coating
Delivery form
Powder
Regional Availability
Chemical Media Resistance
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.
The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.
For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991