View list of

CAMPUS® datasheet | RADIFLAM® A RV350AF


This datasheet of RADIFLAM® A RV350AF from RadiciPlastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  RADIFLAM® A RV350AF | PA66-GF35 FR | RadiciPlastics
Product Texts
DESIGNATION:
Thermoplastics ISO1874-PA66,MFR,-110,GF35

BRIEF DESCRIPTION:
PA66 Flame retardant injection moulding grade
with red phosphorus, halogen free.
35% Glass fibre reinforced, for high stiffness items.
UL94 V0 rated at 0,8mm.
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 10700 / 9050 MPa ISO 527-1/-2
Stress at break 135 / 95 MPa ISO 527-1/-2
Strain at break 2.1 / 2.2 % ISO 527-1/-2
Charpy impact strength (+23°C) 55 / 70 kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 52 / 59 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 11 / 13 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 8.5 / 9 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 260 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 235 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 250 / * °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 245 / * °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. V-0 / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
UL recognition UL / * - -
Burning Behav. at thickness h V-0 / * class IEC 60695-11-10
Thickness tested 0.8 / * mm IEC 60695-11-10
UL recognition UL / * - -
Electrical propertiesdry / condUnitTest Standard
Volume resistivity >1E13 / 1E13 Ohm*m IEC 60093
Surface resistivity * / 1E14 Ohm IEC 60093
Comparative tracking index * / 550 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 5.4 / * % Sim. to ISO 62
Humidity absorption 1.3 / * % Sim. to ISO 62
Density 1480 / * kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Processing conditions acc. ISO 1874 - ISO ....-2
Injection Molding, melt temperature 280 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Diagrams
Viscosity-shear rate , RADIFLAM® A RV350AF, PA66-GF35 FR, RadiciPlastics
Shearstress-shear rate , RADIFLAM® A RV350AF, PA66-GF35 FR, RadiciPlastics
Stress-strain , RADIFLAM® A RV350AF, PA66-GF35 FR, RadiciPlastics
Stress-strain , RADIFLAM® A RV350AF, PA66-GF35 FR, RadiciPlastics
Secant modulus-strain , RADIFLAM® A RV350AF, PA66-GF35 FR, RadiciPlastics
Secant modulus-strain , RADIFLAM® A RV350AF, PA66-GF35 FR, RadiciPlastics
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Lubricants
Regional Availability
Other text information
Injection molding
PREPROCESSING
Max. water content 0.2%
Drying temperature 80°C
Drying time 2-4h (dry air dryer)

PROCESSING
Melt temperature 280°C
Mold temperature 80°C
Disclaimer
This database provides the technical properties
of thermoplastics produced and marketed by
RADICI NOVACIPS
and his subsidiaries companies:

RADILON® A          Polyamide 66
RADILON® S          Polyamide 6
RADILON® CA       Copolyamide 66/6
RADILON® CS       Copolyamide 6 semiaromatic
RADITER® B          Poly(butylene terephthalate)
RADIFLAM® A         Polyamide 66,  self-extinguishing
RADIFLAM® S         Polyamide 6,   self-extinguishing
RADIFLAM® B         Polybutylene terephthalate, self-extinguishing
HERAFLEX® A        Stirenic Thermoplastic Elastomer SEBS
HERAFLEX® E        Ether-Ester Thermoplastic Elastomer
HERAFLEX® B        Stirenic Thermoplastic Elastomer SBS
HERAFLEX® P        Modified Polypropylene
RADILENE® R        Polyethylene and Polypropylene

The data and graphs contained in this database were carried out
by our Research Centers and shall in no event be held to
constitute or imply any warranty, undertaking, express or
implied commitment from our part.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991