View list of

CAMPUS® datasheet | RADILENE® R 70 IF 0 4058 A


This datasheet of RADILENE® R 70 IF 0 4058 A from RadiciPlastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  RADILENE® R 70 IF 0 4058 A | (PE-HD) | RadiciPlastics
Product Texts
No predrying necessary
DESIGNATION
Thermoplastics ISO 1043: HDPE

BRIEF DESCRIPTION
Shore hardness: 61D (3s)
Processable, recyclable, no charged and completely non-toxic
Application examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating and waste pipe)
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 1100 MPa ISO 527-1/-2
Yield stress 20 MPa ISO 527-1/-2
Yield strain 9 % ISO 527-1/-2
Nominal strain at break >50 % ISO 527-1/-2
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 132 °C ISO 11357-1/-3
Other propertiesValueUnitTest Standard
Density 960 kg/m³ ISO 1183
Characteristics
Processing
Other Extrusion, Coating
Delivery form
Pellets
Regional Availability
Disclaimer
This database provides the technical properties
of thermoplastics produced and marketed by
RADICI NOVACIPS
and his subsidiaries companies:

RADILON® A          Polyamide 66
RADILON® S          Polyamide 6
RADILON® CA       Copolyamide 66/6
RADILON® CS       Copolyamide 6 semiaromatic
RADITER® B          Poly(butylene terephthalate)
RADIFLAM® A         Polyamide 66,  self-extinguishing
RADIFLAM® S         Polyamide 6,   self-extinguishing
RADIFLAM® B         Polybutylene terephthalate, self-extinguishing
HERAFLEX® A        Stirenic Thermoplastic Elastomer SEBS
HERAFLEX® E        Ether-Ester Thermoplastic Elastomer
HERAFLEX® B        Stirenic Thermoplastic Elastomer SBS
HERAFLEX® P        Modified Polypropylene
RADILENE® R        Polyethylene and Polypropylene

The data and graphs contained in this database were carried out
by our Research Centers and shall in no event be held to
constitute or imply any warranty, undertaking, express or
implied commitment from our part.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991