DESIGNATION:
Thermoplastics ISO 7792-PBT, MGRS, 09-030

BRIEF DESCRIPTION:
PBT General purpose injection moulding grade.
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 2750 MPa ISO 527-1/-2
Yield stress 60 MPa ISO 527-1/-2
Yield strain 8.5 % ISO 527-1/-2
Nominal strain at break 35 % ISO 527-1/-2
Charpy impact strength (+23°C) N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 4.2 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 4.2 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 225 °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 60 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 165 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 180 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
Volume resistivity 1E12 Ohm*m IEC 60093
Comparative tracking index 550 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.4 % Sim. to ISO 62
Humidity absorption 0.1 % Sim. to ISO 62
Density 1320 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Processing conditions acc. ISO 7792 - ISO ....-2
Injection Molding, melt temperature 245 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 10724
Diagrams
Viscosity-shear rate , RADITER® B N100, PBT, RadiciPlastics
Shearstress-shear rate , RADITER® B N100, PBT, RadiciPlastics
Stress-strain , RADITER® B N100, PBT, RadiciPlastics
Secant modulus-strain , RADITER® B N100, PBT, RadiciPlastics
Specific volume-temperature (pvT) , RADITER® B N100, PBT, RadiciPlastics
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Lubricants
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre-drying recommended.
Max. water content 0.04%
Drying temperature 110°C
Drying time 2-4h (dry air dryer)

PROCESSING
Melt temperature 245°C
Mold temperature 60°C
Disclaimer
This database provides the technical properties
of thermoplastics produced and marketed by
RADICI NOVACIPS
and his subsidiaries companies:

RADILON® A          Polyamide 66
RADILON® S          Polyamide 6
RADILON® CA       Copolyamide 66/6
RADILON® CS       Copolyamide 6 semiaromatic
RADITER® B          Poly(butylene terephthalate)
RADIFLAM® A         Polyamide 66,  self-extinguishing
RADIFLAM® S         Polyamide 6,   self-extinguishing
RADIFLAM® B         Polybutylene terephthalate, self-extinguishing
HERAFLEX® A        Stirenic Thermoplastic Elastomer SEBS
HERAFLEX® E        Ether-Ester Thermoplastic Elastomer
HERAFLEX® B        Stirenic Thermoplastic Elastomer SBS
HERAFLEX® P        Modified Polypropylene
RADILENE® R        Polyethylene and Polypropylene

The data and graphs contained in this database were carried out
by our Research Centers and shall in no event be held to
constitute or imply any warranty, undertaking, express or
implied commitment from our part.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991