View list of
  • All ARKEMA grades
  • All PA12 grades
  • All grades beginning with R

CAMPUS® datasheet | RILSAN AESN O 14 TL


This datasheet of RILSAN AESN O 14 TL from ARKEMA is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  RILSAN AESN O 14 TL | PA12 | ARKEMA
Product Texts
DESIGNATION ISO 1874- PA12, EHLN, 22-010
 RILSAN
 Rigid grade
 Available colour : Transparent
 Light and heat stabilized
 Good abrasion resistance
 Resistance at low temperature
 Suitable for sublimation

 Exemple of applications : Ski top layer
Rheological propertiesdry / condUnitTest Standard
Melt volume-flow rate (MVR) 2.1 / * cm³/10min ISO 1133
Temperature 235 / * °C ISO 1133
Load 5 / * kg ISO 1133
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus - / 1130 MPa ISO 527-1/-2
Yield stress - / 34 MPa ISO 527-1/-2
Yield strain - / 11 % ISO 527-1/-2
Nominal strain at break - / >50 % ISO 527-1/-2
Charpy impact strength (+23°C) N / N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) N / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) - / 63 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) - / 11 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 178 / * °C ISO 11357-1/-3
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 3.2 / * mm IEC 60695-11-10
Other propertiesdry / condUnitTest Standard
Density 1010 / 1010 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 280 °C ISO 294
Injection Molding, mold temperature 50 °C ISO 10724
Injection Molding, pressure at hold 16 MPa ISO 294
Diagrams
Stress-strain , RILSAN AESN O 14 TL, PA12, ARKEMA
Secant modulus-strain , RILSAN AESN O 14 TL, PA12, ARKEMA
Characteristics
Processing
Profile Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Lubricants
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat, Transparent
Regional Availability
Disclaimer

This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991