RILSAN AMV O TLD | PA12 | ARKEMA
Product Texts
DESIGNATION ISO 1874-PA12,MHLR,16-010 RILSAN Rigid grade for injection moulding. Available colour : natural. Light and heat stabilized. Mould-release agent. High impact strength. Easy filling of the mold due to its well adapted viscosity. Low shrinkage : include 1% on average for the design of the mold. Very good dimensionnal stability (low moisture absorption). Example applications : Parts for all technology with high impact strength requirements.
| Rheological properties | dry / cond | Unit | Test Standard |
| Melt volume-flow rate (MVR) | 18 / * | cm³/10min | ISO 1133 |
| Temperature | 235 / * | °C | ISO 1133 |
| Load | 2.16 / * | kg | ISO 1133 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 1400 / 1260 | MPa | ISO 527-1/-2 |
| Yield stress | 44 / 42 | MPa | ISO 527-1/-2 |
| Yield strain | 7 / 7 | % | ISO 527-1/-2 |
| Nominal strain at break | >50 / >50 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | N / N | kJ/m² | ISO 179/1eU |
| Charpy impact strength (-30°C) | N / N | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 5 / 5 | kJ/m² | ISO 179/1eA |
| Charpy notched impact strength (-30°C) | 5 / 6 | kJ/m² | ISO 179/1eA |
| Shore D hardness (15s) | 72 / * | - | ISO 868 |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 178 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (1.80 MPa) | 55 / * | °C | ISO 75-1/-2 |
| Temp. of deflection under load (0.45 MPa) | 135 / * | °C | ISO 75-1/-2 |
| Vicat softening temperature (50°C/h 50N) | 142 / * | °C | ISO 306 |
| Burning Behav. at 1.5 mm nom. thickn. | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 1.6 / * | mm | IEC 60695-11-10 |
| Burning Behav. at thickness h | V-2 / * | class | IEC 60695-11-10 |
| Thickness tested | 3.2 / * | mm | IEC 60695-11-10 |
| Oxygen index | 22 / * | % | ISO 4589-1/-2 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Volume resistivity | - / 1E12 | Ohm*m | IEC 60093 |
| Surface resistivity | * / 1E14 | Ohm | IEC 60093 |
| Electric strength | - / 30 | kV/mm | IEC 60243-1 |
| Comparative tracking index | * / 600 | - | IEC 60112 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 1.6 / * | % | Sim. to ISO 62 |
| Density | 1010 / 1010 | kg/m³ | ISO 1183 |
| Test specimen production | Value | Unit | Test Standard |
| Injection Molding, melt temperature | 270 | °C | ISO 294 |
| Injection Molding, mold temperature | 50 | °C | ISO 10724 |
| Injection Molding, pressure at hold | 16 | MPa | ISO 294 |
Diagrams
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
PREPROCESSING
Max water content: < 0.1 %
Notice text : RILSAN is delivered in sealed bags and is
: ready for use.
: Every opened bag of RILSAN which has not been
: used within two hours must, as a precaution, be
: re-dried.
: Drying conditions are 4 h at 80-90 °C in a
: forced-air oven.
PROCESSING
Melt temperature : 200 - 250 °C
Chemical Media Resistance
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.
The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.
For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991