offers extended functionality!CAMPUS® datasheet | RILSAN BESN NOIR P210 TL
This datasheet of RILSAN BESN NOIR P210 TL from ARKEMA is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
RILSAN BESN NOIR P210 TL | PA11-I | ARKEMA
Product Texts
DESIGNATION ISO 1874-PA11-HIP,EHL,22-005 RILSAN PA11 : produced from a renewable source Flexible grade for tubes extrusion. Available colours : black Ligth and heat stabilized. Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Good chemical resistance. Example applications : Tubes for air brake system.approved by ISO 7628, DIN 73378 (PA11-PHLY), NFR 12632, SAEJ 844. Tubes for diesel and hot diesel circuits.
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | - / 655 | MPa | ISO 527-1/-2 |
| Yield stress | - / 32 | MPa | ISO 527-1/-2 |
| Yield strain | - / 31 | % | ISO 527-1/-2 |
| Nominal strain at break | >50 / >50 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | N / N | kJ/m² | ISO 179/1eU |
| Charpy impact strength (-30°C) | N / N | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | - / 34 | kJ/m² | ISO 179/1eA |
| Charpy notched impact strength (-30°C) | - / 10 | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 182 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (1.80 MPa) | 45 / * | °C | ISO 75-1/-2 |
| Temp. of deflection under load (0.45 MPa) | 110 / * | °C | ISO 75-1/-2 |
| Other properties | dry / cond | Unit | Test Standard |
| Density | 1040 / 1040 | kg/m³ | ISO 1183 |
Characteristics
Processing
Profile Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Lubricants, Plasticizer
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.
The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.
For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991