  RILSAN BESNO P40 W6 TL | PA11 FR(30) | ARKEMA
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus - / 510 MPa ISO 527-1/-2
Yield stress - / 23 MPa ISO 527-1/-2
Yield strain - / 37 % ISO 527-1/-2
Nominal strain at break >50 / >50 % ISO 527-1/-2
Charpy impact strength (+23°C) - / N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) - / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) - / 25 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) - / 3 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 180 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 47 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 130 / * °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-2 / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
UL recognition UL / * - -
Characteristics
Processing
Profile Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Plasticizer
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer

This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991