View list of
  • All ARKEMA grades
  • All PA11 grades
  • All grades beginning with R

CAMPUS® datasheet | RILSAN MB 3504 HP NAT


This datasheet of RILSAN MB 3504 HP NAT from ARKEMA is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  RILSAN MB 3504 HP NAT | PA11 | ARKEMA
Product Texts
DESIGNATION ISO 1874-PA11-HIP, EHL, 22-005
 
 RILSAN PA11 :
 produced from a renewable source

 Flexible grade for tubes extrusion.
 Available colour : natural.
 Light and heat stabilized.

 Flexibility.
 High burst pressure and impact strength.
 Fit for use in a wide range of temperature.
 Good chemical resistance.

 Example applications : Tubes for air brake system.approved by 
 ISO 7628, DIN 73378 (PA11-PHLY), NFR 12632, SAEJ 844.
Rheological propertiesdry / condUnitTest Standard
Melt volume-flow rate (MVR) 1 / * cm³/10min ISO 1133
Temperature 235 / * °C ISO 1133
Load 2.16 / * kg ISO 1133
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 610 / 520 MPa ISO 527-1/-2
Yield stress 32 / 30 MPa ISO 527-1/-2
Yield strain 32 / 33 % ISO 527-1/-2
Nominal strain at break >50 / >50 % ISO 527-1/-2
Charpy impact strength (+23°C) N / N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) N / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 55 / N kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 7 / 10 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 185 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 40 / * °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 3.2 / * mm IEC 60695-11-10
Oxygen index 22 / * % ISO 4589-1/-2
Other propertiesdry / condUnitTest Standard
Density 1030 / 1030 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 270 °C ISO 294
Injection Molding, mold temperature 50 °C ISO 10724
Injection Molding, pressure at hold 16 MPa ISO 294
Diagrams
Viscosity-shear rate , RILSAN MB 3504 HP NAT, PA11, ARKEMA
Shearstress-shear rate , RILSAN MB 3504 HP NAT, PA11, ARKEMA
Dynamic Shear modulus-temperature , RILSAN MB 3504 HP NAT, PA11, ARKEMA
Stress-strain , RILSAN MB 3504 HP NAT, PA11, ARKEMA
Secant modulus-strain , RILSAN MB 3504 HP NAT, PA11, ARKEMA
Stress-strain (isochronous) 23°C, RILSAN MB 3504 HP NAT, PA11, ARKEMA
Creep modulus-time 23°C, RILSAN MB 3504 HP NAT, PA11, ARKEMA
Specific volume-temperature (pvT) , RILSAN MB 3504 HP NAT, PA11, ARKEMA
Characteristics
Processing
Injection Molding, Profile Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Lubricants, Plasticizer
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Profile extrusion

PREPROCESSING

Max water content: < 0.1  %

Notice text      :      RILSAN is delivered in sealed bags and is
                 :      ready for use.

                 :      Every opened bag of RILSAN which has not been
                 :      used within two hours must, as a precaution, be
                 :      re-dried.
                  
                 :      Drying conditions are 4 h at 80-90 °C in a
                 :      forced-air oven.

PROCESSING

Melt temperature : 190 - 250 °C
Disclaimer

This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991