RILSAN MB 3610 NAT | PA11 | ARKEMA
Product Texts
DESIGNATION ISO 1874- PA11-P, EHL, 16-002 RILSAN PA11 : produced from a renewable source High flexible grade for tubes extrusion. Available colours : natural or black (MB 3610 NOIR) Light and heat stabilized. High flexibility. Non blooming High fatigue resistance Very good impact resistance Very good chemical resistance. Example applications : Pneumatic applications
| Rheological properties | dry / cond | Unit | Test Standard |
| Melt volume-flow rate (MVR) | 4 / * | cm³/10min | ISO 1133 |
| Temperature | 235 / * | °C | ISO 1133 |
| Load | 5 / * | kg | ISO 1133 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 225 / 200 | MPa | ISO 527-1/-2 |
| Stress at 50% strain | 20.5 / 20 | MPa | ISO 527-1/-2 |
| Strain at break | >50 / >50 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | N / N | kJ/m² | ISO 179/1eU |
| Charpy impact strength (-30°C) | N / N | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | N / N | kJ/m² | ISO 179/1eA |
| Charpy notched impact strength (-30°C) | 7 / 10 | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 181 / * | °C | ISO 11357-1/-3 |
| Burning Behav. at 1.5 mm nom. thickn. | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 1.6 / * | mm | IEC 60695-11-10 |
| Burning Behav. at thickness h | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 3.2 / * | mm | IEC 60695-11-10 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Volume resistivity | 1.90E11 / - | Ohm*m | IEC 60093 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 1.1 / * | % | Sim. to ISO 62 |
| Humidity absorption | 0.45 / * | % | Sim. to ISO 62 |
| Density | 1030 / 1030 | kg/m³ | ISO 1183 |
Diagrams
Characteristics
Processing
Profile Extrusion
Delivery form
Pellets
Additives
Plasticizer
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Profile extrusion
PREPROCESSING
Max water content: < 0.1 %
Notice text : RILSAN is delivered in sealed bags and is
: ready for use.
: Every opened bag of RILSAN which has not been
: used within two hours must, as a precaution, be
: re-dried.
: Drying conditions are 4 h at 80-90 °C in a
: forced-air oven.
PROCESSING
Melt temperature : 190 - 250 °C
Chemical Media Resistance
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.
The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.
For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991