View list of

CAMPUS® datasheet | SCHULATEC® TinCo 50


This datasheet of SCHULATEC® TinCo 50 from A. Schulman GmbH is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  SCHULATEC® TinCo 50 | PBT-(MF(x)+Z)85 | A. Schulman GmbH
Product Texts
Plastic/metal hybrid based on PA 6 processed like thermoplastics while showing the electrical and electromagnetic properties of metals Specific electrical conductivity: 2 * 10E+5 S/m


Mechanical propertiesValueUnitTest Standard
Tensile Modulus 4300 MPa ISO 527-1/-2
Stress at break 44 MPa ISO 527-1/-2
Strain at break 3.5 % ISO 527-1/-2
Charpy impact strength (+23°C) 31 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 7 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
Volume resistivity 5E-6 Ohm*m IEC 60093
Other propertiesValueUnitTest Standard
Density 3900 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Thermal conductivity of melt 7 W/(m K) -
Characteristics
Processing
Injection Molding
Delivery form
Granules
Additives
Release agent
Regional Availability
Other text information
Injection molding
Pretreatment
Predrying: 2-4 h / 120°C

Processing:

Melttemperature230 - 260°C
Mouldtemperature70 - 90°C

Disclaimer
The properties given in this software are typical, non-binding
mean values found fpor injection moulded natural coloured test
bars. Pigments and other modification may alter these values.
The characteristic values are based on our know-how and experience.
They do not warrant any specific properties. All our products
must be subjected to in house tests and inspections by the user
before application. This applies above all with regard to their
suitability for a particular purpose. It also applies accordingly
for all other written or verbal information given by our personnel.
Our General Terms of Business apply in all other respects,
particulaly with regard to liability for material defects.

If there are questions to given information, to further
properties or further A. Schulman products please contact

                  A. Schulman GmbH
                  Huettenstrasse 211
                  50170 Kerpen
                  Tel: 02273 / 561-0
                  Contact: Dipl.-Ing. M. Berg
                           aschulman@de.aschulman.com