View list of
  • All Polimeri grades
  • All ABS grades
  • All grades beginning with S

CAMPUS® datasheet | SINKRAL® C 442


This datasheet of SINKRAL® C 442 from Polimeri Europa is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  SINKRAL® C 442 | ABS | Polimeri Europa
Product Texts
Symbol according to ISO 1043-1: ABS

Designation: Thermoplastics ISO 2580-ABS 1,MGN,105-08-16-20

SINKRAL C 442 is a heat resistant injection moulding grade offering good flow and impact resistance together with an excellent thermal stability during its processing.


Applications:

Thanks to its low Yellow Index and its colour constancy, it is suitable for self-colouring, mainly in the automotive industry for interior (extruded profiles, interior trims,..) and, with proper masterbatches, for exterior parts such as grilles and rear view mirrors.

Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 6 cm³/10min ISO 1133
Temperature 220 °C ISO 1133
Load 10 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 2400 MPa ISO 527-1/-2
Yield stress 48 MPa ISO 527-1/-2
Yield strain 3 % ISO 527-1/-2
Nominal strain at break 30 % ISO 527-1/-2
Charpy impact strength (+23°C) N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 100 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 14 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 7 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Glass transition temperature (10°C/min) 110 °C ISO 11357-1/-2
Temp. of deflection under load (1.80 MPa) 85 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 106 °C ISO 306
Coeff. of linear therm. expansion (parallel) 90 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm IEC 60695-11-10
UL recognition UL - -
Electrical propertiesValueUnitTest Standard
Relative permittivity (1MHz) 3.1 - IEC 60250
Dissipation factor (1MHz) 150 E-4 IEC 60250
Volume resistivity 1E13 Ohm*m IEC 60093
Surface resistivity 1E14 Ohm IEC 60093
Electric strength 30 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.6 % Sim. to ISO 62
Humidity absorption 0.2 % Sim. to ISO 62
Density 1040 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 960 kg/m³ -
Spec. heat capacity melt 2150 J/(kg K) -
Test specimen productionValueUnitTest Standard
Processing conditions acc. ISO 2580 - ISO ....-2
Injection Molding, melt temperature 250 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 70 MPa ISO 294
Diagrams
Viscosity-shear rate , SINKRAL® C 442, ABS, Polimeri
Shearstress-shear rate , SINKRAL® C 442, ABS, Polimeri
Dynamic Shear modulus-temperature , SINKRAL® C 442, ABS, Polimeri
Stress-strain , SINKRAL® C 442, ABS, Polimeri
Secant modulus-strain , SINKRAL® C 442, ABS, Polimeri
Specific volume-temperature (pvT) , SINKRAL® C 442, ABS, Polimeri
Spec. enthalpy/mass-temp. (DSC) , SINKRAL® C 442, ABS, Polimeri
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
0 Injection Molding
PREPROCESSING

Drying conditions:

    Drying temperature                80 °C

    Drying time                          2- 4 h

    Maximum water content         0.2 %



PROCESSING

Typical pro cessing temperature range:

    Melt temperature         230 - 270 °C

    Mold temperature          40  - 70 °C

Profile extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2- 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

Sheet extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2- 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

Disclaimer
Dear CAMPUS User,

The data, information and suggestions are provided for guidance
purpose only.
The Company accepts no responsibility for the results obtained
therefrom, as neither for their utilisation in infringement of
possible patents rights.
All indicated data refer to natural grades.
On the subject of the experimental products, the Company reserves the
right to change without prewarning the characteristics, to optimise
the performances.

If you have any questions regarding CAMPUS, please send
an e-mail to:Pe Campus


For further information regarding Polimeri Europa:
	Polimeri Europa Homepage


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.