  Sorona® FG3015G NC010 | PBT-GF15 | DuPont Engineering Polymers
Product Texts
DuPont™ Sorona® EP thermoplastic polymers contain between 20 and 37% renewably sourced material (by weight) derived from corn. The new material exhibits performance and molding characteristics similar to high-performance PBT (polybutylene terephtalate).

 

In addition to good strength and stiffness, early tests indicate improved surface appearance, lower warpage and good dimensional stability, making it very attractive in a range of uses for automotive parts and components, electrical and electronics as well as industrial and consumer products.

 

DuPont™ Sorona® EP thermoplastic polymers are derived from corn with DuPont Tate & Lyle Susterra™ renewably sourced propanediol as key intermediate. The exact percentage of renewably sourced content for each commercial product is available on the renewable.dupont.com website.

 

Sorona® EP thermoplastic polymer starts with the same basic polymer chemistry as Sorona® polymer used for fibers but through proprietary formulation technology, further enhancements are added to create high-performance resins suitable for engineering plastics applications.

 

______________________________________________________


Sorona® FG3015G is a 15% glass reinforced, 31% renewably sourced polytrimethylene terephtalate resin for injection molding. It is specifically suitable for the food industry.

Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 13 cm³/10min ISO 1133
Temperature 250 °C ISO 1133
Load 2.16 kg ISO 1133
Molding shrinkage (parallel) 0.3 % ISO 294-4, 2577
Molding shrinkage (normal) 0.7 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 6500 MPa ISO 527-1/-2
Stress at break 120 MPa ISO 527-1/-2
Strain at break 2.5 % ISO 527-1/-2
Charpy impact strength (+23°C) 25 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 5.5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 227 °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 200 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 223 °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm IEC 60695-11-10
Other propertiesValueUnitTest Standard
Density 1440 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 1250 kg/m³ -
Diagrams
Viscosity-shear rate , Sorona® FG3015G NC010, PBT-GF15, DuPont
Shearstress-shear rate , Sorona® FG3015G NC010, PBT-GF15, DuPont
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Regional Availability
Other text information
Injection molding

PREPROCESSING


Drying Recommended = Yes
Drying Temperature = 120°C
Drying Time, Dehumidified Dryer = 4h
Processing Moisture Content = < 0.02 %


PROCESSING


Melt Temperature Optimum = 260°C
Melt Temperature Range = 250-270°C
Mold Temperature Optimum = 100°C
Mold Temperature Range = 80-110°C


Moulding guide

Chemical Media Resistance
Acids
Acetic Acid (5% by mass) (23°C)
Citric Acid solution (10% by mass) (23°C)
Lactic Acid (10% by mass) (23°C)
Hydrochloric Acid (36% by mass) (23°C)
Nitric Acid (40% by mass) (23°C)
Sulfuric Acid (38% by mass) (23°C)
Sulfuric Acid (5% by mass) (23°C)
Chromic Acid solution (40% by mass) (23°C)
Bases
Sodium Hydroxide solution (35% by mass) (23°C)
Sodium Hydroxide solution (1% by mass) (23°C)
Ammonium Hydroxide solution (10% by mass) (23°C)
Alcohols
Isopropyl alcohol (23°C)
Methanol (23°C)
Ethanol (23°C)
Hydrocarbons
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Ketones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Mineral oils
SAE 10W40 multigrade motor oil (23°C)
SAE 10W40 multigrade motor oil (130°C)
SAE 80/90 hypoid-gear oil (130°C)
Insulating Oil (23°C)
Standard Fuels
ISO 1817 Liquid 1 (60°C)
ISO 1817 Liquid 2 (60°C)
ISO 1817 Liquid 3 (60°C)
ISO 1817 Liquid 4 (60°C)
Standard fuel without alcohol (pref. ISO 1817 Liquid C) (23°C)
Standard fuel with alcohol (pref. ISO 1817 Liquid 4) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (90°C)
Diesel fuel (pref. ISO 1817 Liquid F) (>90°C)
Salt solutions
Sodium Chloride solution (10% by mass) (23°C)
Sodium Hypochlorite solution (10% by mass) (23°C)
Sodium Carbonate solution (20% by mass) (23°C)
Sodium Carbonate solution (2% by mass) (23°C)
Zinc Chloride solution (50% by mass) (23°C)
Other
Ethyl Acetate (23°C)
Hydrogen peroxide (23°C)
DOT No. 4 Brake fluid (130°C)
Ethylene Glycol (50% by mass) in water (108°C)
1% nonylphenoxy-polyethyleneoxy ethanol in water (23°C)
50% Oleic acid + 50% Olive Oil (23°C)
Water (23°C)
Deionized water (90°C)
Phenol solution (5% by mass) (23°C)
Disclaimer

E.I. du Pont de Nemours and Company is pleased to provide information about its products with the CAMPUS electronic database.

The information provided is gratis and DuPont assumes no obligation or liability for any advice furnished or for any results obtained with respect to this information.

All such advice is given and accepted at the risk of the buyer. The disclosure of information herein is not an express or implied license to operate under any patent of DuPont or others.

DuPont warrants that the use or sale of any material which is described herein and is offered for sale by DuPont does not infringe any patent covering the material itself, but does not warrant against infringement by reason of the use thereof in combination with other materials or the operation of any process.

Unless otherwise noted, the property values are for natural color (NC010) resins only. Colorants or other additives may alter some or all of the properties.
The data listed herein fall within the normal range of product properties and they should not be used to establish specification limits nor used alone as the basis of design.

Material Safety Data Sheets (SDSs) can be obtained from local sales offices.

Products listed herein should not be used in medical applications involving permanent implantation in the human body or contact with internal body fluids or tissues unless the material has been provided from DuPont under a written contract that is consistent with DuPont policy regarding medical applications and expressly acknowledges the contemplated use.

For further information, please contact your DuPont representative.

You may also request a copy of DuPont policy regarding medical applications H-50103-2 and DuPont caution regarding medical applications H-50102-2.

Products listed herein may from time to time be modified or removed.
Please call your local sales office to determine current availability.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991