View list of
  • All DSM grades
  • All PA46 grades
  • All grades beginning with S

CAMPUS® datasheet | Stanyl® TE373


This datasheet of Stanyl® TE373 from DSM Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Stanyl® TE373 | PA46 | DSM Engineering Plastics
Product Texts
Heat Stabilized, Wear and Friction Modified

ISO 1043 PA46

Welcome to the astonishing world of Stanyl®
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 2800 / 1000 MPa ISO 527-1/-2
Yield stress 85 / 50 MPa ISO 527-1/-2
Yield strain 10 / 20 % ISO 527-1/-2
Nominal strain at break 10 / 15 % ISO 527-1/-2
Charpy impact strength (+23°C) 150 / N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 105 / 120 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 5 / 10 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 4 / 4 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 295 / * °C ISO 11357-1/-3
Glass transition temperature (10°C/min) 75 / * °C ISO 11357-1/-2
Temp. of deflection under load (1.80 MPa) 190 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 85 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 110 / * E-6/K ISO 11359-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 12.4 / * % Sim. to ISO 62
Humidity absorption 3.4 / * % Sim. to ISO 62
Density 1170 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
Viscosity number 180 / * cm³/g ISO 307, 1157, 1628
Rheological calculation propertiesValueUnitTest Standard
Density of melt 1000 kg/m³ -
Thermal conductivity of melt 0.253 W/(m K) -
Spec. heat capacity melt 2780 J/(kg K) -
Eff. thermal diffusivity 8.96E-8 m²/s -
Diagrams
Dynamic Shear modulus-temperature , Stanyl® TE373, PA46, DSM
Specific volume-temperature (pvT) , Stanyl® TE373, PA46, DSM
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
Disclaimer
 All information supplied by or on behalf of DSM in relation to its
products, whether in the nature of data, recommendations or otherwise,
is supported by research and, in good faith, believed reliable, but DSM
assumes no liability and makes no warranties of any kind, express or
implied, including, but not limited to, those of title, merchantability,
fitness for a particular purpose or non-infringement or any warranty
arising from a course of dealing, usage, or trade practice whatsoever
in respect of application, processing or use made of the aforementioned
information or product. The user assumes all responsibility for the use
of all information provided and shall verify quality and other properties or
any consequence from the use of all such information.

Typical values are indicative only and are not to be construed as being
binding specifications.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991