This datasheet of Styrolux® 3G 55 from Styrolution Group GmbH is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
Styrolux® 3G 55 | SB | Styrolution Group GmbH
Product Texts
Styrolux® 3G 55 is a clear styrene-butadiene copolymer (SBC) used mainly in sheet extrusion and thermoforming applications. Styrolux® 3G 55 is specifically designed for improved performance in blends with general-purpose polystyrene, providing parts with an excellent balance of toughness, transparency and economics. Because of the tendency of blocking, Styrolux® 3G 55 is mainly used in inline thermoforming. Styrolux® 3G 55 is difficult to print and decorate since it contains a microcrystalli
ne wax.
Major applications include the whole array of food and non-food packagings, CAP/MAP, drink cups, caps, lids, deli-trays, shrink and labelling film.
Major applications include the whole array of food and non-food packagings, CAP/MAP, drink cups, caps, lids, deli-trays, shrink and labelling film.
| Rheological properties | Value | Unit | Test Standard |
| Melt volume-flow rate, MVR | 14 | cm³/10min | ISO 1133 |
| Temperature | 200 | °C | ISO 1133 |
| Load | 5 | kg | ISO 1133 |
| Mechanical properties | Value | Unit | Test Standard |
| Tensile Modulus | 900 | MPa | ISO 527-1/-2 |
| Yield stress | 15 | MPa | ISO 527-1/-2 |
| Yield strain | 2 | % | ISO 527-1/-2 |
| Nominal strain at break | >50 | % | ISO 527-1/-2 |
| Charpy impact strength, +23°C | N | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength, +23°C | 85 | kJ/m² | ISO 179/1eA |
| Thermal properties | Value | Unit | Test Standard |
| Temp. of deflection under load, 1.80 MPa | 51 | °C | ISO 75-1/-2 |
| Temp. of deflection under load, 0.45 MPa | 62 | °C | ISO 75-1/-2 |
| Vicat softening temperature, 50°C/h 50N | 35 | °C | ISO 306 |
| Coeff. of linear therm. expansion, parallel | 75 | E-6/K | ISO 11359-1/-2 |
| Burning Behav. at 1.5 mm nom. thickn. | HB | class | IEC 60695-11-10 |
| Thickness tested | 1.6 | mm | IEC 60695-11-10 |
| Electrical properties | Value | Unit | Test Standard |
| Relative permittivity, 100Hz | 2.5 | - | IEC 60250 |
| Relative permittivity, 1MHz | 2.5 | - | IEC 60250 |
| Dissipation factor, 100Hz | 3 | E-4 | IEC 60250 |
| Dissipation factor, 1MHz | 8 | E-4 | IEC 60250 |
| Volume resistivity | >1E13 | Ohm*m | IEC 60093 |
| Surface resistivity | >1E15 | Ohm | IEC 60093 |
| Comparative tracking index | 600 | - | IEC 60112 |
| Other properties | Value | Unit | Test Standard |
| Water absorption | 0.07 | % | Sim. to ISO 62 |
| Humidity absorption | 0.07 | % | Sim. to ISO 62 |
| Density | 1010 | kg/m³ | ISO 1183 |
| Test specimen production | Value | Unit | Test Standard |
| Injection Molding, melt temperature | 230 | °C | ISO 294 |
| Injection Molding, mold temperature | 50 | °C | ISO 10724 |
| Injection Molding, injection velocity | 200 | mm/s | ISO 294 |
Characteristics
Processing
Film Extrusion, Sheet Extrusion, Other Extrusion, Blow Molding
Regional Availability
Other text information
Film extrusion
PROCESSING
Extrusion, Blown film, Melt temperature: 180 °C
Extrusion, Flat film, Melt temperature: 190 - 230 °C
Extrusion, Blown film, Melt temperature: 180 °C
Extrusion, Flat film, Melt temperature: 190 - 230 °C
Other extrusion
PROCESSING
Extrusion, Pipes, Melt temperature: 230 °C
Extrusion, Pipes, Melt temperature: 230 °C
Sheet extrusion
PROCESSING
Extrusion, Plates, Melt temperature: 190 °C
Extrusion, Plates, Melt temperature: 190 °C
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact
Styrolution GmbH
Styrolution Infopoint
mailto:styrenics.infopoint@basf.com
Tel: +49 621 60 41446
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact
Styrolution GmbH
Styrolution Infopoint
mailto:styrenics.infopoint@basf.com
Tel: +49 621 60 41446
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012