  TROGAMID® CX9701 nc (nf) | PAIND/INDT | Evonik Industries AG
Product Texts
TROGAMID® CX9701 nc


High viscosity extrusion resin with external feeding aid

  • microcrystalline
  • permanently transparent
  • chemical and stress crack resistant
  • high impact resistance
  • outstanding UV and light stability
  • low water absorption
  • dimensionally stable.
     
Application examples: Lamp profile and covers, anti-graffiti coatings.
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 14 cm³/10min ISO 1133
Temperature 285 °C ISO 1133
Load 5 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 1400 MPa ISO 527-1/-2
Yield stress 60 MPa ISO 527-1/-2
Yield strain 8 % ISO 527-1/-2
Nominal strain at break >50 % ISO 527-1/-2
Tensile creep modulus (1h) 1400 MPa ISO 899-1
Tensile creep modulus (1000h) 700 MPa ISO 899-1
Charpy impact strength (+23°C) N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 16 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 14 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 250 °C ISO 11357-1/-3
Glass transition temperature (10°C/min) 140 °C ISO 11357-1/-2
Temp. of deflection under load (1.80 MPa) 108 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 122 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 130 °C ISO 306
Coeff. of linear therm. expansion (parallel) 90 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 90 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
Relative permittivity (100Hz) 3.6 - IEC 60250
Relative permittivity (1MHz) 3.2 - IEC 60250
Dissipation factor (100Hz) 115 E-4 IEC 60250
Dissipation factor (1MHz) 325 E-4 IEC 60250
Volume resistivity >1E13 Ohm*m IEC 60093
Surface resistivity 1E13 Ohm IEC 60093
Electric strength 27 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 3.5 % Sim. to ISO 62
Density 1020 kg/m³ ISO 1183
Material specific propertiesValueUnitTest Standard
Viscosity number 155 cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 280 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 70 MPa ISO 294
Diagrams
Stress-strain (isochronous) 23°C, TROGAMID® CX9701 nc (nf), PAIND/INDT, Evonik Degussa
Creep modulus-time 23°C, TROGAMID® CX9701 nc (nf), PAIND/INDT, Evonik Degussa
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Sheet Extrusion, Other Extrusion, Blow Molding, Thermoforming
Delivery form
Pellets
Additives
Lubricants
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Transparent
Regional Availability
Other text information
Injection molding


PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is

dependent on the drying temperature. In practice a drying time of 6-12 hours at a temperature

of 100 - 120°C  (depending on the water content of the resin) has been found to be satisfactory.
With the exception of fresh air dryers, all conventional dryers can be used.

PROCESSING INFORMATION

Melt Temperature:280 - 300°C
Mold Temperature:60 - 100°C
Film extrusion

PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is

dependent on the drying temperature. In practice a drying time of 6-12 hours at a temperature

of 100 - 120°C (depending on the water content of the resin) has been found to be satisfactory.
With the exception of fresh air dryers, all conventional dryers can be used.


PROCESSING INFORMATION
Melt Temperature : 280 - 300 °C

Other extrusion

PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is

dependent on the drying temperature. In practice a drying time of 6-12 hours at a temperature

of 100 - 120°C (depending on the water content of the resin) has been found to be satisfactory.
With the exception of fresh air dryers, all conventional dryers can be used.


PROCESSING INFORMATION
Melt Temperature : 280 - 300 °C

Profile extrusion

PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is

dependent on the drying temperature. In practice a drying time of 6-12 hours at a temperature

of 100 - 120°C (depending on the water content of the resin) has been found to be satisfactory.
With the exception of fresh air dryers, all conventional dryers can be used.


PROCESSING INFORMATION
Melt Temperature : 280 - 300 °C

Sheet extrusion

PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is

dependent on the drying temperature. In practice a drying time of 6-12 hours at a temperature

of 100 - 120°C (depending on the water content of the resin) has been found to be satisfactory.
With the exception of fresh air dryers, all conventional dryers can be used.


PROCESSING INFORMATION
Melt Temperature : 280 - 300 °C

Blow molding

PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is

dependent on the drying temperature. In practice a drying time of 6-12 hours at a temperature

of 100 - 120°C (depending on the water content of the resin) has been found to be satisfactory.
With the exception of fresh air dryers, all conventional dryers can be used.


PROCESSING INFORMATION

Melt Temperature :280 - 300°C
Disclaimer
With the following data, which reflect our current knowledge and experience,
we wish to describe possible applications, however this information is given
without guarantee or assurance of the appropriate properties for a specific
application.

The processor is not relieved of the responsibility for incoming quality control
nor from his own testing and analysis.

All data concerning product safety (EG-guideline, BGVV, FDA) are of principle
nature and can be limitied regarding migration, temperature and type of food.
They reflect the status as of Feb. 29, 2012. To insure that this data reflects the
current state, please contact our Product Safety Department.

Should you have any questions, wishes or suggestions about CAMPUS,
please refer to the following address:

  Link to Evonik Industries AG homepage

In any case, we hope you enjoy working with CAMPUS!

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991