  Technyl® 2710IR | PA66-I | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide 66, impact modified, fast cycle time, for injection molding.

 

TECHNYL® 2710IR is used in all sectors of industry, offering an excellent productivity.

 

This grade is widely used for

- Battery gasket, Fastener

 

This product is available in natural color and in colors on request

 
Mechanical propertiesdry / condUnitTest Standard
Yield stress 65 / - MPa ISO 527-1/-2
Yield strain 25 / - % ISO 527-1/-2
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 262 / * °C ISO 11357-1/-3
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 3.2 / * mm IEC 60695-11-10
Oxygen index 21 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
Relative permittivity (1MHz) 3.2 / 3.2 - IEC 60250
Dissipation factor (1MHz) 0.02 / 0.1 E-4 IEC 60250
Volume resistivity >1E13 / 1E13 Ohm*m IEC 60093
Surface resistivity * / 1E14 Ohm IEC 60093
Electric strength 30 / 16 kV/mm IEC 60243-1
Comparative tracking index 550 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.1 / * % Sim. to ISO 62
Density 1110 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, mold temperature 80 °C ISO 10724
Characteristics
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content less than 0.2% with a dehumidified air drying equipment at approx.80°C

 

Recommended moulding conditions:

 

- Barrel temperatures : - feed zone 265~270°C

- compression zone 270~280°C

- front zone 280~290°C

- Mould temperatures: 60~ 80°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991