View list of
  • All Rhodia grades
  • All PA66 grades
  • All grades beginning with T

CAMPUS® datasheet | Technyl® A 208F


This datasheet of Technyl® A 208F from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® A 208F | PA66 | Rhodia Polyamide Engineering Plastics
Product Texts
Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection moulding.


TECHNYL A 208F offers three main advantages: excellent filling qualities, good long term thermal properties and is V2 rated under 0.4 mm. according to UL94. It is particularly suitable for the moulding of long parts with thin wall sections requiring good thermal resistance:

- cable ties and fasteners

- connectors

This product is available in black.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 3200 / 1600 MPa ISO 527-1/-2
Yield stress 85 / 50 MPa ISO 527-1/-2
Yield strain 7 / 10 % ISO 527-1/-2
Charpy impact strength (+23°C) N / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 4.5 / 8 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 263 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 75 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 210 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 70 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h V-2 / * class IEC 60695-11-10
Thickness tested 0.4 / * mm IEC 60695-11-10
Oxygen index 26 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
Relative permittivity (100Hz) 4.1 / 6 - IEC 60250
Relative permittivity (1MHz) 2.9 / 3.2 - IEC 60250
Dissipation factor (100Hz) 200 / 800 E-4 IEC 60250
Dissipation factor (1MHz) 300 / 800 E-4 IEC 60250
Volume resistivity 1E13 / 1E12 Ohm*m IEC 60093
Surface resistivity * / 1E12 Ohm IEC 60093
Electric strength 27 / 26 kV/mm IEC 60243-1
Comparative tracking index 475 / 500 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.2 / * % Sim. to ISO 62
Density 1140 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
Viscosity number 140 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 225 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Diagrams
Viscosity-shear rate , Technyl® A 208F, PA66, Rhodia
Shearstress-shear rate , Technyl® A 208F, PA66, Rhodia
Stress-strain , Technyl® A 208F, PA66, Rhodia
Specific volume-temperature (pvT) , Technyl® A 208F, PA66, Rhodia
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
Recommended moulding conditions:

Barrel temperatures:

- feed zone 270 - 275°C

- compression zone 280 - 285°C

- front zone 285 - 290°C

Mould temperatures: 60 at 80°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991