CAMPUS® datasheet | Technyl® A 218 V30 Black 34NG-K


This datasheet of Technyl® A 218 V30 Black 34NG-K from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® A 218 V30 Black 34NG-K | PA66-GF30 | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide 66, reinforced with 30% of glass fibre, for injection moulding specially stabilized to improve its resistance to automotive cooling liquids.

 

Technyl A218V30 bk 34NG-K is particularly recommended for the injection moulding of parts in permanent contact with cooling liquids in cars, such as:

Cooling and heating radiator systems, header tanks, thermostat components, and inlet/outlet pipes

 

This product is available in Black and in color on request.

Thermal propertiesValueUnitTest Standard
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
UL recognition UL - -
Oxygen index 23 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
Relative permittivity (1MHz) 3.7 - IEC 60250
Dissipation factor (1MHz) 100 E-4 IEC 60250
Volume resistivity 1E13 Ohm*m IEC 60093
Surface resistivity 6E14 Ohm IEC 60093
Comparative tracking index 450 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1370 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, mold temperature 80 °C ISO 10724
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding

The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content less than 0,2% with a dehumidified air drying equipment at approx.80°C

 

Recommended moulding conditions:

- Barrel temperatures:  - feed zone                  260~270°C

                                 - compression zone      270~280°C

                                 - front zone                   280~290°C

- Mould temperatures:                                    80°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.