This datasheet of Technyl® A 218HP V50 black 21N from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® A 218HP V50 black 21N | PA66-GF50 | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide 66, reinforced with 50% of glass fibre, heat stabilized, for injection moulding.

 

TECHNYL® A 218HP V50 BLACK 21N offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature.

 

Offering an excellent combination between thermal and mechanical properties, it is used in all sectors of industry, such as in the automotive for engine components and in the electrical field for bobbin coil formers.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 15000 / 10500 MPa ISO 527-1/-2
Stress at break 200 / 143 MPa ISO 527-1/-2
Strain at break 2 / 2 % ISO 527-1/-2
Charpy impact strength (+23°C) 85 / 94 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 17 / 23 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 263 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 253 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 260 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Density 1520 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
Viscosity number 97 / * cm³/g ISO 307, 1157, 1628
Diagrams
Stress-strain , Technyl® A 218HP V50 black 21N, PA66-GF50, Rhodia
Secant modulus-strain , Technyl® A 218HP V50 black 21N, PA66-GF50, Rhodia
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content of less than 0,12% with a dehumidified air drying equipment at approx 80°C.

 

Recommended moulding conditions:

 

Barrel temperatures: - feed zone 260 - 270°C

- compression zone 270 - 280 °C

- front zone 280 - 290°C

Mould temperatures: 60 at 100°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991