This datasheet of Technyl® A 218W V33 Natural T from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® A 218W V33 Natural T | PA66-GF33 | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide PA66, translucent, reinforced with 33% of glass fibre, heat stabilized, for injection moulding.

 

TECHNYL® A 218W V33 NATURAL T is particularly recommended for the injection moulding of parts in permanent contact with cooling liquids in cars, such as: - cooling and heating radiator systems, header tanks, fluid reservoir, thermostat components , inlet / outlet pipes.

 

This product is available in natural.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 10200 / - MPa ISO 527-1/-2
Stress at break 190 / - MPa ISO 527-1/-2
Strain at break 3.8 / - % ISO 527-1/-2
Charpy impact strength (+23°C) 90.7 / - kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 11 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 263 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 250 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Density 1400 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
Viscosity number 145 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
Injection Molding, mold temperature 80 °C ISO 10724
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat, Transparent
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content less than 0.2% with a dehumidified air drying equipment at approx 80°C.

 

Recommended moulding conditions:

 

- Barrel temperatures:

- feed zone 255-265°C

- compressio n zone 265-275°C

- front zone 275-280°C

 

- Mould temperatures: 60-80°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991