  Technyl® A 30G1 | PA66 FR | Rhodia Polyamide Engineering Plastics
Product Texts
Flame retardant Polyamide 66, unreinforced, heat stabilised, for injection moulding.

 

This flame retardant grade, UL 94 V-0 (0.4 mm), GWIT 850°C (0,8 mm) offers best in class flammability performance combined with excellent impact and strain properties. It is particularly suitable for moulding electrical components such as connections, junction blocks, terminal blocks and connectors.

 

This product is also suitable for use in electrical appliances needing to comply with the IEC 60335-1 regulation.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 2800 / - MPa ISO 527-1/-2
Charpy impact strength (+23°C) 110 / * kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 5.8 / * kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 250 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 85 / * °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
UL recognition UL / * - -
Burning Behav. at thickness h V-0 / * class IEC 60695-11-10
Thickness tested 0.4 / * mm IEC 60695-11-10
UL recognition UL / * - -
Electrical propertiesdry / condUnitTest Standard
Comparative tracking index 250 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Density 1320 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, mold temperature 80 °C ISO 10724
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content of less than 0,2% with a dehumidified air drying equipment at approx 80°C.

 

Recommended moulding conditions:

 

Barrel temperatures :

 

- feed zone 270 - 270°C

- compression zone 260 - 280°C

- front zone 270 - 290°C

 

Mould temperatures: 60 at 80°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991