This datasheet of Technyl® A 52 G1 MX 20 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
Technyl® A 52 G1 MX 20 | PA66-MF | Rhodia Polyamide Engineering Plastics
Product Texts
is a Polyamide 6.6 glow wire resistant , reinforced with mineral filler
Colors: it is marketed in black color.
TECHNYL A 52 G1 MX20 features the following properties:
• Glow wire resistant
• Good finishing
• Good dimensional stability
TECHNYL A 52 G1 MX20 is indicated for pieces with low warping and good behaviour at fire, as for example, circuit breakers (IEC NBR 60898) and boxes of fusers
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 6800 / - | MPa | ISO 527-1/-2 |
| Stress at break | 60 / - | MPa | ISO 527-1/-2 |
| Strain at break | 1.3 / - | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 25 / * | kJ/m² | ISO 179/1eU |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 260 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (1.80 MPa) | 165 / * | °C | ISO 75-1/-2 |
| Temp. of deflection under load (0.45 MPa) | 230 / * | °C | ISO 75-1/-2 |
| Burning Behav. at 1.5 mm nom. thickn. | V-2 / * | class | IEC 60695-11-10 |
| Thickness tested | 1.6 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Other properties | dry / cond | Unit | Test Standard |
| Density | 1350 / - | kg/m³ | ISO 1183 |
| Test specimen production | Value | Unit | Test Standard |
| Injection Molding, mold temperature | 80 | °C | ISO 10724 |
Other text information
Injection molding
To injection mould TECHNYL A 52 G1 MX20 , we suggest the following machine regulations:
• Cylinder Temperature:
feeding zone: 235º - 240º C
compression zone: 240° - 245°C
mixing zone: 245° - 250°C
nozzle: 260º - 275ºC
• Mould Temperature: 60-80ºC
Disclaimer
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991