View list of
CAMPUS® datasheet | Technyl® A 548B2 V15 Black 23N
This datasheet of Technyl® A 548B2 V15 Black 23N from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
Technyl® A 548B2 V15 Black 23N | PA66-GF15 | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide PA66, reinforced with 15% of glass fibres, heat stabilised, with a very high viscosity for blowmoulding.
Thanks to its excellent thermal resistance, TECHNYL® A548B2 V15 BLACK 23N can be used to produce air ducts for turbo charged engines. Furthermore, this grade, due to the superior resistance to the automotive cooling circuit liquids, can be used for the production of coolant system pipes.
The product is available in black colour
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 4900 / 3500 | MPa | ISO 527-1/-2 |
| Stress at break | 90 / 57 | MPa | ISO 527-1/-2 |
| Strain at break | 4.7 / 8.8 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 65 / 79 | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 13.5 / - | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 260 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (1.80 MPa) | 210 / * | °C | ISO 75-1/-2 |
| Other properties | dry / cond | Unit | Test Standard |
| Density | 1200 / - | kg/m³ | ISO 1183 |
Diagrams
Characteristics
Processing
Blow Molding
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to final moisture content less than 0.1% with a dehumidified air drying equipment at approx. 80°C.
Recommended extrusion conditions:
Barrel Feed zone 255-265 °C
Barrel Compression zone 260-270 °C
Barrel Front Zone 260-270 °C
Accumulator 260-270 °C
Die Temperature 260-270 °C
Melt Temperature 265-280 °C
Drying Temperature 70-80 °C
Drying Time 6-8 h Desiccant dryer Dew Point -30 °C
Mould Temperature 60-90 °C
Disclaimer
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991