This datasheet of Technyl® A 60 G2 V30 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy.
This product is ideally suited for large and small appliances and connectic applications requiring glow wire no flame performance. This product is registered at the VDE institute for the IEC 60335 normative in all colour references down to 0.8mm thickness. It has a robust GWIT/GWT pass with excellent CTI (>550V) and ball pressure test performance (>150°C).
This product is available in Natural, Grey and Black. Specific colours and Laser Marking grades optimised for YAG and UV laser types are also available upon request.
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 11500 / - | MPa | ISO 527-1/-2 |
| Stress at break | 150 / - | MPa | ISO 527-1/-2 |
| Strain at break | 2.5 / - | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 55 / * | kJ/m² | ISO 179/1eU |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 262 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (1.80 MPa) | 247 / * | °C | ISO 75-1/-2 |
| Temp. of deflection under load (0.45 MPa) | 256 / * | °C | ISO 75-1/-2 |
| Burning Behav. at 1.5 mm nom. thickn. | V-0 / * | class | IEC 60695-11-10 |
| Thickness tested | 1.6 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Burning Behav. at thickness h | V-0 / * | class | IEC 60695-11-10 |
| Thickness tested | 0.8 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Electrical properties | dry / cond | Unit | Test Standard |
| Comparative tracking index | 550 / - | - | IEC 60112 |
| Other properties | dry / cond | Unit | Test Standard |
| Density | 1460 / - | kg/m³ | ISO 1183 |
| Test specimen production | Value | Unit | Test Standard |
| Injection Molding, mold temperature | 80 | °C | ISO 10724 |
Recommended moulding conditions :
Barrel temperatures:
- feed zone 260 - 270°C
- compression zone 260 - 270°C
- front zone 260 - 270°C
Mould temperatures: 60 - 80°C
For products containing Flame additives Rhodia recomends the use of a CR19% C1.9% coating for the steels to prolong the life time of the processing equipment.
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.