This datasheet of Technyl® A 60G1 V30 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® A 60G1 V30 | PA66-GF30 FR | Rhodia Polyamide Engineering Plastics
Product Texts

Flame retardant Polyamide PA66 reinforced with 30% of glass fibre, for injection moulding.


This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This product is ideally suited for industrial controls and power distribution applications such as MCBs and contactors.

 

The long term thermal performance of this grade also make it ideal for under-the-bonnet Auto applications where it can withstand temperatures of 160°C for over 6000hrs. The thermal ageing value for this product in accordance to the IEC 216 RTI are the following;

 

-Impact 160°C @ 6000hrs & 140 @ 20000hrs

-Strength 165°C @ 6000hrs & 145 @ 20000hrs

-Dielectric 160°C @ 6000hrs & 145 @ 20000hrs

 

This product is available in Natural, Grey and Black. Specific colours and Laser Marking grades optimised for YAG and UV laser types are also available upon request.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 11000 / 8000 MPa ISO 527-1/-2
Stress at break 148 / 115 MPa ISO 527-1/-2
Strain at break 2.3 / 4.2 % ISO 527-1/-2
Charpy impact strength (+23°C) 58 / 75 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 6.7 / 8.5 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 263 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 245 / * °C ISO 75-1/-2
Burning Behav. at thickness h V-0 / * class IEC 60695-11-10
Thickness tested 0.4 / * mm IEC 60695-11-10
Burning Behav. 5V at thickness h 5VA / * class IEC 60695-11-20
Thickness tested 1.6 / * mm IEC 60695-11-20
Oxygen index 33 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 0.73 / * % Sim. to ISO 62
Density 1460 / - kg/m³ ISO 1183
Diagrams
Stress-strain , Technyl® A 60G1 V30, PA66-GF30 FR, Rhodia
Specific volume-temperature (pvT) , Technyl® A 60G1 V30, PA66-GF30 FR, Rhodia
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed

moisture, it must be dried to a final moisture content of less than 0,2% with a dehumidified air drying equipment

at approx 80°C.

Recommended moulding conditions :

Barrel temperatures:

- feed zone 260 - 270°C

- compression zone 260 - 270°C

- front zone 260 - 270°C

Mould temperatures: 60 - 80°C

For products containing Flame additives Rhodia recomends the use of a CR19% C1.9% coating for the steels

to prolong the life time of the processing equipment.

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991