View list of
  • All Rhodia grades
  • All PA66 grades
  • All grades beginning with T

CAMPUS® datasheet | Technyl® A 718 V30


This datasheet of Technyl® A 718 V30 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® A 718 V30 | PA66-GF30 | Rhodia Polyamide Engineering Plastics
Product Texts
is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moulding

 

Color: it is sailed on natural and black color

 

TECHNYL A 718 V30 features the following properties:

 

• Good mechanical properties

• Great superficial aspect

• Dimensional stability

• Excellent flow characteristics

 

This product is indicated for pieces with complex geometries, which need an excellent superficial aspect and good mechanical properties.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 9000 / - MPa ISO 527-1/-2
Stress at break 150 / - MPa ISO 527-1/-2
Strain at break 2.5 / - % ISO 527-1/-2
Charpy impact strength (+23°C) 35 / * kJ/m² ISO 179/1eU
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 255 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 250 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 0.5 / * % Sim. to ISO 62
Density 1370 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding

 

To injection mold TECHNYL A 718 V30 we suggest the following machine regulations:

 

Cylinder Temperature:

feeding zone: 250° - 270°C

compression zone: 260° - 280°C

mixing zone: 270° - 290°C

nozzle: 260º - 280°C

 

Mold Temperature: 60° - 80°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991