  Technyl® AFX 218 V60 | PA66-GF60 | Rhodia Polyamide Engineering Plastics
Product Texts
High Flow Polyamide 66 reinforced with 60% of glass fibre, heat stabilized, for injection moulding.
Rheological propertiesdry / condUnitTest Standard
Molding shrinkage (parallel) 0.3 / * % ISO 294-4, 2577
Molding shrinkage (normal) 0.4 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 22000 / 18000 MPa ISO 527-1/-2
Stress at break 268 / 195 MPa ISO 527-1/-2
Strain at break 2.1 / 3.1 % ISO 527-1/-2
Charpy impact strength (+23°C) 18 / 22 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 98 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 264 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 257 / * °C ISO 75-1/-2
Electrical propertiesdry / condUnitTest Standard
Volume resistivity >1E13 / - Ohm*m IEC 60093
Electric strength 40 / - kV/mm IEC 60243-1
Comparative tracking index 550 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Humidity absorption 0.6 / * % Sim. to ISO 62
Density 1690 / - kg/m³ ISO 1183
Diagrams
Stress-strain , Technyl® AFX 218 V60, PA66-GF60, Rhodia
Stress-strain , Technyl® AFX 218 V60, PA66-GF60, Rhodia
Secant modulus-strain , Technyl® AFX 218 V60, PA66-GF60, Rhodia
Secant modulus-strain , Technyl® AFX 218 V60, PA66-GF60, Rhodia
Specific volume-temperature (pvT) , Technyl® AFX 218 V60, PA66-GF60, Rhodia
Characteristics
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content less than 0.2% with a dehumidified air drying equipment at approx. 80°C.

 

Recommended moulding conditions:

 

-Barrel temperatures:

 

-feed zone                  260-270°C

-compression zone     270-280°C

-front zone                 280-290°C

-Mould temperatures: 60-90°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991