  Technyl® AR 130/GF BLACK | PA66-GF30 | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide PA66 reinforced with 30% of glass fibre. heat stabilised, containing recycled material.
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 9500 / - MPa ISO 527-1/-2
Stress at break 133 / - MPa ISO 527-1/-2
Strain at break 2.5 / - % ISO 527-1/-2
Charpy impact strength (+23°C) 43 / - kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 5.4 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 260 / * °C ISO 11357-1/-3
Other propertiesdry / condUnitTest Standard
Density 1370 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 240 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 10724
Diagrams
Stress-strain , Technyl® AR 130/GF BLACK, PA66-GF30, Rhodia
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding
PROCESSING
Melt temperature: 260°C
Mold temperature: 80°C
Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991