CAMPUS® datasheet | Technyl® C 236SI


This datasheet of Technyl® C 236SI from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® C 236SI | PA6 | Rhodia Polyamide Engineering Plastics
Product Texts
Unreinforced polyamide 6 with high impact strength for injection moulding.

 

TECHNYL® C 236SI has high impact strength and flexibility.

 

This grade is suitable for power tools, sports goods, furniture and machine components.

 

This product is available in natural, black and in colours on request.

Rheological propertiesdry / condUnitTest Standard
Molding shrinkage (parallel) 1.9 / * % ISO 294-4, 2577
Molding shrinkage (normal) 1.5 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 2200 / 910 MPa ISO 527-1/-2
Yield stress 54 / - MPa ISO 527-1/-2
Yield strain 4 / - % ISO 527-1/-2
Charpy impact strength (+23°C) N / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 76 / N kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 16 / * kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 220 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 56 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 1.27 / * % Sim. to ISO 62
Density 1090 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, mold temperature 80 °C ISO 10724
Diagrams
Stress-strain , Technyl® C 236SI, PA6, Rhodia
Secant modulus-strain , Technyl® C 236SI, PA6, Rhodia
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content of less than 0,2% with a dehumidified air drying equipment at approx 80°C.

 

Recommended moulding conditions:

 

Barrel temperatures

 

- feed zone 240 - 280°C

- compression zone 240 - 280°C

- front zone 260 - 280°C

 

Mould temperatures 80°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.