  Technyl® C 246SI V30 | PA6-GF30 | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide 6, reinforced with 30 % of glass fibre, with high impact resistance, for injection moulding.

 

Having good mechanical properties, this grade is used in all sectors of industry.

 

This product is available in natural and black.

Rheological propertiesdry / condUnitTest Standard
Molding shrinkage (parallel) 0.3 / * % ISO 294-4, 2577
Molding shrinkage (normal) 0.8 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 8300 / 4900 MPa ISO 527-1/-2
Stress at break 140 / 90 MPa ISO 527-1/-2
Strain at break 4.5 / 10 % ISO 527-1/-2
Charpy impact strength (+23°C) 92 / * kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 23 / 36 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 15 / 15 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 222 / * °C ISO 11357-1/-3
Other propertiesdry / condUnitTest Standard
Water absorption 0.88 / * % Sim. to ISO 62
Density 1320 / - kg/m³ ISO 1183
Diagrams
Stress-strain , Technyl® C 246SI V30, PA6-GF30, Rhodia
Stress-strain , Technyl® C 246SI V30, PA6-GF30, Rhodia
Secant modulus-strain , Technyl® C 246SI V30, PA6-GF30, Rhodia
Secant modulus-strain , Technyl® C 246SI V30, PA6-GF30, Rhodia
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to final moisture content less than 0.2% with a dehumidified air drying equipment at approx. 80°C.

 

Recommended moulding conditions:

 

- Barrel temperatures:

 

feed zone 250 - 280°C

compression zone 250 - 280°C

front zone 260 - 290°C

 

- Mould temperature: 70 - 90 °C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991