This datasheet of Technyl® C 52G1 MX 25 Grey 7035 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
Technyl® C 52G1 MX 25 Grey 7035 | PA6-MF25 | Rhodia Polyamide Engineering Plastics
Product Texts
Flame retardant polyamide PA6 reinforced with mineral filler for injection moulding, also suitable for thin wall parts.
This phosphorus and halogen free flame retardant grade is particularly suitable for equipment with robust glow wire resistance such as MCB housings.
This grade is available in grey colour.
| Rheological properties | dry / cond | Unit | Test Standard |
| Molding shrinkage (parallel) | 1.1 / * | % | ISO 294-4, 2577 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 6130 / 4000 | MPa | ISO 527-1/-2 |
| Stress at break | 70 / 55 | MPa | ISO 527-1/-2 |
| Strain at break | 2 / 4 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 30 / 50 | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 3 / 6 | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 220 / * | °C | ISO 11357-1/-3 |
| Burning Behav. at 1.5 mm nom. thickn. | V-2 / * | class | IEC 60695-11-10 |
| Thickness tested | 1.6 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Burning Behav. at thickness h | V-2 / * | class | IEC 60695-11-10 |
| Thickness tested | 0.8 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Oxygen index | 29 / * | % | ISO 4589-1/-2 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Comparative tracking index | 600 / - | - | IEC 60112 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 1.1 / * | % | Sim. to ISO 62 |
| Test specimen production | Value | Unit | Test Standard |
| Injection Molding, mold temperature | 80 | °C | ISO 10724 |
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content of less than 0,2% with a dehumidified air drying equipment at approx 80°C.
Recommended moulding conditions :
Barrel temperatures :
- feed zone 220 - 230°C
-compression zone 230 - 240°C
-front zone 245 - 255°C
Mould temperatures : 80°C
Disclaimer
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991