FREE DOWNLOAD
Interested inPrinting Curve Points?
The CAMPUS desktop version
offers extended functionality!CAMPUS® datasheet | Technyl® C 52G1 V25
This datasheet of Technyl® C 52G1 V25 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
TECHNYL® C 52G1 V25 is used in all sectors of industry, offering good glow wireperformance and heat resistance and productivity.
This grade is specifically suited for
- contactors and switches
This product is available in grey colour and in colors on request.
| Rheological properties | dry / cond | Unit | Test Standard |
| Molding shrinkage (parallel) | 0.8 / * | % | ISO 294-4, 2577 |
| Molding shrinkage (normal) | 0.6 / * | % | ISO 294-4, 2577 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 6850 / 4350 | MPa | ISO 527-1/-2 |
| Stress at break | 85 / 51 | MPa | ISO 527-1/-2 |
| Strain at break | 2.7 / 4.2 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 41 / 84 | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 3.5 / 8.6 | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 220 / * | °C | ISO 11357-1/-3 |
| Burning Behav. at 1.5 mm nom. thickn. | V-2 / * | class | IEC 60695-11-10 |
| Thickness tested | 1.6 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Burning Behav. at thickness h | V-2 / * | class | IEC 60695-11-10 |
| Thickness tested | 0.8 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Oxygen index | 33 / * | % | ISO 4589-1/-2 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Comparative tracking index | 550 / - | - | IEC 60112 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 1.1 / * | % | Sim. to ISO 62 |
| Density | 1350 / - | kg/m³ | ISO 1183 |
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content less than 0.2% with a dehumidified air drying equipment at approx.80°C
Recommended moulding conditions:
- Mould
-Barrel temperatures: -feed zone 230 ~ 240°C
-compression zone 235 ~ 245°C
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.