This datasheet of Technyl® C 52G4 MZ25 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® C 52G4 MZ25 | PA6-MF25 FR | Rhodia Polyamide Engineering Plastics
Product Texts
Flame retardant polyamide PA6 reinforced with mineral filler, for injection moulding. Enhanced processing behavior for thin wall parts. 

 

This phosphorus and halogen free flame retardant grade is particularly suitable for equipment with robust glowwire resistance such as MCB housings.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 6400 / - MPa ISO 527-1/-2
Stress at break 75 / - MPa ISO 527-1/-2
Strain at break 3 / - % ISO 527-1/-2
Charpy impact strength (+23°C) 47 / - kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 3 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 222 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 130 / * °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-2 / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
UL recognition UL / * - -
Burning Behav. at thickness h V-2 / * class IEC 60695-11-10
Thickness tested 0.8 / * mm IEC 60695-11-10
UL recognition UL / * - -
Oxygen index 31 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
Comparative tracking index 525 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1 / * % Sim. to ISO 62
Density 1370 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, mold temperature 80 °C ISO 10724
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content of less than 0,2% with a dehumidified air drying equipment at approx 80°C.

 

Recommended moulding conditions :

 

Barrel temperatures :

- feed zone 220 - 230°C

-compre ssion zone 230 - 240°C

-front zone 245 - 255°C

 

Mould temperatures : 80°C

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991