This datasheet of Technyl® C 536XT from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Technyl® C 536XT | PA6-I | Rhodia Polyamide Engineering Plastics
Product Texts
Unreinforced polyamide 6, with high viscosity and high toughness, for extrusion blow moulding.

 

TECHNYL C 536XT is suitable for blow moulding applications.

 

TECHNYL C 536XT is characterised by good processing behaviour, impact resistance even at low temperature and high barrier properties especially to fluids such as fuels and oils.

 

TECHNYL C 536XT is recommended for use in applications such as tanks, bottles, tubes or pipes.

 

This product is available in natural and black.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 2200 / 910 MPa ISO 527-1/-2
Yield stress 54 / - MPa ISO 527-1/-2
Yield strain 4 / - % ISO 527-1/-2
Charpy impact strength (+23°C) N / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 76 / N kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 16 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 220 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 56 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 1.27 / * % Sim. to ISO 62
Density 1090 / - kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Technyl® C 536XT, PA6-I, Rhodia
Shearstress-shear rate , Technyl® C 536XT, PA6-I, Rhodia
Characteristics
Processing
Blow Molding
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. Although the material is delivered dry, it is recommended to dry the material to a final moisture content less than 0.08% with a dehumidified air drying equipment at approx. 80°C.

 

Recommended processing conditions :

 

Feed zone : 240 – 250°C

Compression zone : 230 – 250°C

Front zone : 230 – 250°C

Die temperature : 230 – 260°C

Tool temperature : 60 – 80°C

 

The material is delivered in airtight packaging, ready for use.

Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991