CAMPUS® datasheet | Technyl® CR 218 V30 black 1 N
This datasheet of Technyl® CR 218 V30 black 1 N from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
Technyl® CR 218 V30 black 1 N | PA6-GF30 | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide PA6 reinforced with 30% of glass fibre, heat stabilised, containing recycled material.
This grade is suitable for none critical and less demanding parts.
This product is available in black.
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 9600 / - | MPa | ISO 527-1/-2 |
| Stress at break | 140 / - | MPa | ISO 527-1/-2 |
| Strain at break | 2 / - | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 50 / - | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 5.2 / - | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 222 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (1.80 MPa) | 208 / * | °C | ISO 75-1/-2 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Relative permittivity (1MHz) | 3.71 / - | - | IEC 60250 |
| Other properties | dry / cond | Unit | Test Standard |
| Density | 1360 / - | kg/m³ | ISO 1183 |
| Material specific properties | dry / cond | Unit | Test Standard |
| Viscosity number | 145 / * | cm³/g | ISO 307, 1157, 1628 |
Diagrams
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content less than 0.2% with a dehumidified air drying equipment at approx. 80°C.
Recommended moulding conditions :
- Barrel temperatures :
feed zone 225 - 230°C
Disclaimer
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.