This datasheet of Technyl® D 247F from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
Technyl® D 247F | (PA66+PA610)-I | Rhodia Polyamide Engineering Plastics
Product Texts
Polyamide 66 & 610, impact modified, alkali resistance, mold release, for injection molding.
TECHNYL® D 247 F is used in all sectors of industry, offering high impact strength & excellent productivity.
This product is especially suitable for the following purposes:
- Battery gasket
This product is available in natural colors on request
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 262 / * | °C | ISO 11357-1/-3 |
| Burning Behav. at thickness h | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 3.2 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Other properties | dry / cond | Unit | Test Standard |
| Density | 1080 / - | kg/m³ | ISO 1183 |
| Test specimen production | Value | Unit | Test Standard |
| Injection Molding, mold temperature | 80 | °C | ISO 10724 |
Other text information
Injection molding
The material is supplied in airtight bags, ready for use. In the case that the virgin material has absorbed moisture, it must be dried to a final moisture content less than 0,2% with a dehumidified air drying equipment at approximately 80°C.
Recommended moulding conditions:
-Barrel temperatures
Feed zone 265~270°C
Compression zone 270~280°C
Front zone 280~290°C
-Mould temperatures 60~80°C
Disclaimer
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991