  Terblend® N NM-13 | (ABS+PA6) | Styrolution Group GmbH
Product Texts
Terblend® N NM-13 is an ABS/PA blend combining excellent impact strength at low temperatures with easy processability and good surface appearance.
Rheological propertiesdry / condUnitTest Standard
Melt volume-flow rate, MVR 25 / * cm³/10min ISO 1133
Temperature 240 / * °C ISO 1133
Load 10 / * kg ISO 1133
Molding shrinkage, parallel 0.7 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.8 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 1600 / 1100 MPa ISO 527-1/-2
Yield stress 35 / - MPa ISO 527-1/-2
Yield strain 3.4 / - % ISO 527-1/-2
Nominal strain at break >50 / - % ISO 527-1/-2
Charpy impact strength, +23°C N / - kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 80 / - kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 30 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Temp. of deflection under load, 1.80 MPa 58 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 80 / * °C ISO 75-1/-2
Vicat softening temperature, 50°C/h 50N 91 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 100 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
Electrical propertiesdry / condUnitTest Standard
Relative permittivity, 1MHz 2.9 / 3.3 - IEC 60250
Dissipation factor, 1MHz 150 / 550 E-4 IEC 60250
Volume resistivity >1E13 / 1E11 Ohm*m IEC 60093
Surface resistivity * / 1E14 Ohm IEC 60093
Other propertiesdry / condUnitTest Standard
Humidity absorption 1.1 / * % Sim. to ISO 62
Density 1070 / - kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 928 kg/m³ -
Thermal conductivity of melt 0.156 W/(m K) -
Spec. heat capacity of melt 2410 J/(kg K) -
Ejection temperature 90 °C -
Diagrams
Stress-strain , Terblend® N NM-13, (ABS+PA6), Styrolution
Secant modulus-strain , Terblend® N NM-13, (ABS+PA6), Styrolution
Tensile modulus-temperature , Terblend® N NM-13, (ABS+PA6), Styrolution
Characteristics
Processing
Injection Molding
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 240 - 270 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.

In order to check the availability of products please contact us or our
sales agency.


For more information about our products contact

Styrolution GmbH
Styrolution Infopoint
mailto:styrenics.infopoint@basf.com
Tel: +49 621 60 41446

CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012