This datasheet of Ultradur® B 2550 FC from BASF is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  Ultradur® B 2550 FC | PBT | BASF
Product Texts
The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including FDA, European Food Contact n°2002/72/EC and GMP (EC) n°2023/2006.

Additional food contact compliances may also be available. Please contact your local representative or plastics safety (E-Mail: plastics.safety@basf.com, Fax: +49 621-60-93253).

Abbreviated designation according to ISO 1043-1: PBT
CLASSIFICATION ACCORDING TO ISO 7792-1:
Moulding Compound ISO 7792-PBT, M+H+LGHLN, 11-030
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 40 cm³/10min ISO 1133
Temperature 250 °C ISO 1133
Load 2.16 kg ISO 1133
Molding shrinkage (parallel) 1.6 % ISO 294-4, 2577
Molding shrinkage (normal) 1.9 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 2500 MPa ISO 527-1/-2
Yield stress 57 MPa ISO 527-1/-2
Yield strain 3.7 % ISO 527-1/-2
Nominal strain at break 35 % ISO 527-1/-2
Tensile creep modulus (1h) 1500 MPa ISO 899-1
Tensile creep modulus (1000h) 1100 MPa ISO 899-1
Charpy impact strength (+23°C) 250 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 6 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 4 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 223 °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 65 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 165 °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 145 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.4 mm IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
Relative permittivity (100Hz) 3.3 - IEC 60250
Relative permittivity (1MHz) 3.3 - IEC 60250
Dissipation factor (100Hz) 13 E-4 IEC 60250
Dissipation factor (1MHz) 200 E-4 IEC 60250
Volume resistivity >1E13 Ohm*m IEC 60093
Surface resistivity 1E13 Ohm IEC 60093
Electric strength 40 kV/mm IEC 60243-1
Comparative tracking index 500 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.5 % Sim. to ISO 62
Humidity absorption 0.25 % Sim. to ISO 62
Density 1300 kg/m³ ISO 1183
Material specific propertiesValueUnitTest Standard
Viscosity number 107 cm³/g ISO 307, 1157, 1628
Rheological calculation propertiesValueUnitTest Standard
Ejection temperature 160 °C -
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 260 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Diagrams
Viscosity-shear rate , Ultradur® B 2550 FC, PBT, BASF
Shearstress-shear rate , Ultradur® B 2550 FC, PBT, BASF
Stress-strain , Ultradur® B 2550 FC, PBT, BASF
Secant modulus-strain , Ultradur® B 2550 FC, PBT, BASF
Stress-strain (isochronous) 23°C, Ultradur® B 2550 FC, PBT, BASF
Creep modulus-time 23°C, Ultradur® B 2550 FC, PBT, BASF
Stress-strain (isochronous) 60°C, Ultradur® B 2550 FC, PBT, BASF
Creep modulus-time 60°C, Ultradur® B 2550 FC, PBT, BASF
Stress-strain (isochronous) 100°C, Ultradur® B 2550 FC, PBT, BASF
Creep modulus-time 100°C, Ultradur® B 2550 FC, PBT, BASF
Specific volume-temperature (pvT) , Ultradur® B 2550 FC, PBT, BASF
Tensile modulus-temperature , Ultradur® B 2550 FC, PBT, BASF
Characteristics
Processing
Injection Molding, Coating
Delivery form
Pellets
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 245 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 70 °C
injection molding, Mold temperature, recommended: 60 °C
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.

In order to check the availability of products please contact us or our
sales agency.


For more information about our products contact your local BASF
representative or

BASF SE
Dept. KS/KC
Fax: 0621-60-49497
e-mail: e-mail

CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991