CAMPUS® datasheet | Ultraform® N2640 Z2


This datasheet of Ultraform® N2640 Z2 from BASF is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  Ultraform® N2640 Z2 | (POM+PUR) | BASF
Product Texts
Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.

Abbreviated designation according to ISO 1043: POM-HI
Designation according to ISO 9988-1: POM-K, M-GNPR,03-001
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 7 cm³/10min ISO 1133
Temperature 190 °C ISO 1133
Load 2.16 kg ISO 1133
Molding shrinkage (parallel) 1.9 % ISO 294-4, 2577
Molding shrinkage (normal) 1.9 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 2000 MPa ISO 527-1/-2
Yield stress 50 MPa ISO 527-1/-2
Yield strain 12 % ISO 527-1/-2
Nominal strain at break 45 % ISO 527-1/-2
Tensile creep modulus (1h) 1550 MPa ISO 899-1
Tensile creep modulus (1000h) 1050 MPa ISO 899-1
Charpy impact strength (+23°C) N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 230 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 11 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 6.5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 167 °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 85 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 150 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 140 °C ISO 306
Coeff. of linear therm. expansion (parallel) 130 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
UL recognition UL - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
Relative permittivity (100Hz) 4 - IEC 60250
Relative permittivity (1MHz) 4 - IEC 60250
Dissipation factor (100Hz) 100 E-4 IEC 60250
Dissipation factor (1MHz) 140 E-4 IEC 60250
Volume resistivity 1E12 Ohm*m IEC 60093
Surface resistivity 1E14 Ohm IEC 60093
Electric strength 40 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.8 % Sim. to ISO 62
Humidity absorption 0.2 % Sim. to ISO 62
Density 1370 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Ejection temperature 105 °C -
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 200 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Diagrams
Viscosity-shear rate , Ultraform® N2640 Z2, (POM+PUR), BASF
Shearstress-shear rate , Ultraform® N2640 Z2, (POM+PUR), BASF
Dynamic Shear modulus-temperature , Ultraform® N2640 Z2, (POM+PUR), BASF
Stress-strain , Ultraform® N2640 Z2, (POM+PUR), BASF
Secant modulus-strain , Ultraform® N2640 Z2, (POM+PUR), BASF
Stress-strain (isochronous) 23°C, Ultraform® N2640 Z2, (POM+PUR), BASF
Creep modulus-time 23°C, Ultraform® N2640 Z2, (POM+PUR), BASF
Stress-strain (isochronous) 40°C, Ultraform® N2640 Z2, (POM+PUR), BASF
Creep modulus-time 40°C, Ultraform® N2640 Z2, (POM+PUR), BASF
Stress-strain (isochronous) 80°C, Ultraform® N2640 Z2, (POM+PUR), BASF
Creep modulus-time 80°C, Ultraform® N2640 Z2, (POM+PUR), BASF
Specific volume-temperature (pvT) , Ultraform® N2640 Z2, (POM+PUR), BASF
Tensile modulus-temperature , Ultraform® N2640 Z2, (POM+PUR), BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 215 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.

In order to check the availability of products please contact us or our
sales agency.


For more information about our products contact your local BASF
representative or

BASF SE
Dept. KS/KC
Fax: 0621-60-49497
e-mail: e-mail

CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991