This datasheet includes:

  Ultramid® Seal-Fit | PA666... | BASF
Product Texts
Transparent, tough, amorphous copolyamide for injection moulding, specially developed for tight overmoulding of metal inlays.
Rheological propertiesdry / condUnitTest Standard
Melt volume-flow rate (MVR) 120 / * cm³/10min ISO 1133
Temperature 275 / * °C ISO 1133
Load 5 / * kg ISO 1133
Molding shrinkage (parallel) 0.3 / * % ISO 294-4, 2577
Molding shrinkage (normal) 0.3 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 2500 / - MPa ISO 527-1/-2
Thermal propertiesdry / condUnitTest Standard
Temp. of deflection under load (0.45 MPa) 57 / * °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 68 / * °C ISO 306
Coeff. of linear therm. expansion (parallel) 100 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 100 / * E-6/K ISO 11359-1/-2
Electrical propertiesdry / condUnitTest Standard
Volume resistivity - / 9E12 Ohm*m IEC 60093
Surface resistivity * / >1E15 Ohm IEC 60093
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Humidity absorption 4.75 / * % Sim. to ISO 62
Density 1100 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
Viscosity number 125 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 250 °C ISO 294
Injection Molding, mold temperature 40 °C ISO 10724
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Transparent
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 60 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 230 - 260 °C
injection molding, Melt temperature, recommended: 240 °C
injection molding, Mold temperature, range: 20 - 50 °C
injection molding, Mold temperature, recommended: 40 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.

In order to check the availability of products please contact us or our
sales agency.


For more information about our products contact your local BASF
representative or

BASF SE
Dept. KS/KC
Fax: 0621-60-49497
e-mail: e-mail

CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991