CAMPUS® datasheet | Ultrason® E 6020 P


This datasheet of Ultrason® E 6020 P from BASF is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  Ultrason® E 6020 P | PESU | BASF
Product Texts
Polyethersulfone flakes, e.g. for membrane applications and coatings.
Abbreviated designation according to ISO 1043-1: PESU
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus - / 2700 MPa ISO 527-1/-2
Yield stress - / 90 MPa ISO 527-1/-2
Yield strain - / 6.7 % ISO 527-1/-2
Charpy impact strength (+23°C) - / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) - / 7.5 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Glass transition temperature (10°C/min) 225 / * °C ISO 11357-1/-2
Temp. of deflection under load (1.80 MPa) 207 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Humidity absorption 1 / * % Sim. to ISO 62
Material specific propertiesdry / condUnitTest Standard
Viscosity number 82 / * cm³/g ISO 307, 1157, 1628
Characteristics
Delivery form
Powder
Regional Availability
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.

In order to check the availability of products please contact us or our
sales agency.


For more information about our products contact your local BASF
representative or

BASF SE
Dept. KS/KC
Fax: 0621-60-49497
e-mail: e-mail

CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991