View list of

CAMPUS® datasheet | VESTAMID L-R3-EP blk (sw)


This datasheet of VESTAMID L-R3-EP blk (sw) from Evonik Industries AG is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  VESTAMID® L-R3-EP blk (sw) | PA12 | Evonik Industries AG
Product Texts
VESTAMID® L-R3-EP blk

 

Resin:                        ISO 1874-PA12-P, EHZ, 22-007  

 

Former Designation: VESTAMID® X3680 sw (t)

 

High viscosity, plasticized electrically conductive PA 12 resin for extrusion. The electrical

resistance values which can be achieved the finished moulding depend on the processing

conditions.

 

Application examples: Pipes and tubes for explosion hazard areas (paint spray installations)

Rheological propertiesdry / condUnitTest Standard
Melt volume-flow rate (MVR) 140 / * cm³/10min ISO 1133
Temperature 275 / * °C ISO 1133
Load 21.6 / * kg ISO 1133
Molding shrinkage (parallel) 1.3 / * % ISO 294-4, 2577
Molding shrinkage (normal) 1.3 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 800 / 750 MPa ISO 527-1/-2
Stress at 50% strain 46 / 46 MPa ISO 527-1/-2
Strain at break >50 / >50 % ISO 527-1/-2
Charpy impact strength (+23°C) N / N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) N / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 38 / 21 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 4 / 5 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 176 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 60 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 120 / * °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 140 / * °C ISO 306
Coeff. of linear therm. expansion (parallel) 150 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 140 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 3.2 / * mm IEC 60695-11-10
Electrical propertiesdry / condUnitTest Standard
Volume resistivity 10 / - Ohm*m IEC 60093
Other propertiesdry / condUnitTest Standard
Humidity absorption 0.5 / * % Sim. to ISO 62
Density 1170 / 1170 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 940 kg/m³ -
Thermal conductivity of melt 0.16 W/(m K) -
Spec. heat capacity melt 2550 J/(kg K) -
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 240 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 70 MPa ISO 294
Characteristics
Processing
Injection Molding, Profile Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Lubricants, Plasticizer
Special Characteristics
Increased electrical conductivity, Anti-static, Light stabilized or stable to light, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding


PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is dependent

on the drying temperature. At a drying temperature of 80°C we recommend, depending on the water

content, a drying time of 8 - 16 hours. Fresh air dryers are acceptable, better would be a dry air or

vacuum dryer. Please note our product literature, plasticized resins can lose plasticizer du ring drying.

PROCESSING INFORMATION

Melt Temperature:220 - 250°C
Mold Temperature:30 - 100°C
Other extrusion

PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is dependent

on the drying temperature. At a drying temperature of 80°C we recommend, depending on the water

content, a drying time of 8 - 16 hours. Fresh air dryers are acceptable, better would be a dry air or

vacuum dryer. Please note our product literature, plasticized resins can lose plasticizer during drying.


PROCESSING INFORMATION
Melt Temperature : 220 - 250 °C

Profile extrusion

PREPROCESSING INFORMATION
Maximum Water Content: 0.1 %
When the indicated water content is exceeded, the resin must be dried. The drying time is dependent

on the drying temperature. At a drying temperature of 80°C we recommend, depending on the water

content, a drying time of 8 - 16 hours. Fresh air dryers are acceptable, better would be a dry air or

vacuum dryer. Please note our product literature, plasticized resins can lose plasticizer during drying.


PROCESSING INFORMATION
Melt Temperature : 220 - 250 °C

Disclaimer
With the following data, which reflect our current knowledge and experience,
we wish to describe possible applications, however this information is given
without guarantee or assurance of the appropriate properties for a specific
application.

The processor is not relieved of the responsibility for incoming quality control
nor from his own testing and analysis.

All data concerning product safety (EG-guideline, BGVV, FDA) are of principle
nature and can be limitied regarding migration, temperature and type of food.
They reflect the status as of Feb. 29, 2012. To insure that this data reflects the
current state, please contact our Product Safety Department.

Should you have any questions, wishes or suggestions about CAMPUS,
please refer to the following address:

  Link to Evonik Industries AG homepage

In any case, we hope you enjoy working with CAMPUS!